material

NaLi2Sb

ID:

mp-5077

DOI:

10.17188/1262793


Tags: Dilithium sodium antimonide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.577 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.28 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.680 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 1 0> <1 1 0> 0.000 198.9
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.000 243.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.004 187.6
Cu (mp-30) <1 0 0> <1 0 0> 0.004 234.5
CdS (mp-672) <1 1 0> <1 1 0> 0.004 198.9
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.007 132.6
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.009 162.4
CdS (mp-672) <0 0 1> <1 1 1> 0.010 243.7
GaN (mp-804) <0 0 1> <1 1 1> 0.013 81.2
InP (mp-20351) <1 1 0> <1 1 0> 0.019 198.9
InP (mp-20351) <1 1 1> <1 1 1> 0.020 243.7
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.020 281.3
GaN (mp-804) <1 1 0> <1 1 0> 0.023 265.3
Au (mp-81) <1 1 0> <1 1 0> 0.026 198.9
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.027 281.3
CsI (mp-614603) <1 1 0> <1 1 0> 0.035 265.3
SiC (mp-11714) <0 0 1> <1 0 0> 0.040 328.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.042 328.2
CaF2 (mp-2741) <1 1 1> <1 1 0> 0.051 265.3
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.058 81.2
Ag (mp-124) <1 1 0> <1 1 0> 0.058 198.9
GaP (mp-2490) <1 1 1> <1 1 0> 0.061 265.3
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.072 331.6
InAs (mp-20305) <1 0 0> <1 0 0> 0.074 187.6
C (mp-66) <1 0 0> <1 0 0> 0.078 234.5
TiO2 (mp-390) <1 1 0> <1 1 0> 0.081 265.3
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.083 187.6
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.086 234.5
Mg (mp-153) <1 1 0> <1 1 0> 0.090 265.3
Si (mp-149) <1 0 0> <1 0 0> 0.090 234.5
BN (mp-984) <1 0 0> <1 0 0> 0.092 234.5
NdGaO3 (mp-3196) <1 0 1> <1 1 1> 0.098 162.4
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.105 331.6
SiC (mp-8062) <1 0 0> <1 0 0> 0.110 93.8
LiF (mp-1138) <1 1 0> <1 1 0> 0.117 265.3
Cu (mp-30) <1 1 0> <1 1 0> 0.123 198.9
TiO2 (mp-390) <1 0 0> <1 0 0> 0.125 187.6
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.130 187.6
KP(HO2)2 (mp-23959) <1 0 0> <1 0 0> 0.131 234.5
NaCl (mp-22862) <1 1 1> <1 0 0> 0.136 281.3
PbS (mp-21276) <1 1 0> <1 1 0> 0.147 198.9
PbS (mp-21276) <1 1 1> <1 1 1> 0.152 243.7
Si (mp-149) <1 1 1> <1 1 0> 0.154 265.3
WS2 (mp-224) <1 0 1> <1 1 0> 0.156 331.6
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.158 331.6
CeO2 (mp-20194) <1 1 1> <1 1 0> 0.159 265.3
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.171 132.6
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.172 331.6
CdS (mp-672) <1 0 0> <1 0 0> 0.174 140.7
CdSe (mp-2691) <1 0 0> <1 0 0> 0.180 187.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
49 20 20 0 0 0
20 49 20 0 0 0
20 20 49 0 0 0
0 0 0 31 0 0
0 0 0 0 31 0
0 0 0 0 0 31
Compliance Tensor Sij (10-12Pa-1)
26.5 -7.6 -7.6 0 0 0
-7.6 26.5 -7.6 0 0 0
-7.6 -7.6 26.5 0 0 0
0 0 0 32.6 0 0
0 0 0 0 32.6 0
0 0 0 0 0 32.6
Shear Modulus GV
24 GPa
Bulk Modulus KV
29 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
29 GPa
Shear Modulus GVRH
23 GPa
Bulk Modulus KVRH
29 GPa
Elastic Anisotropy
0.68
Poisson's Ratio
0.19

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
9.26 0.00 0.00
0.00 9.26 0.00
0.00 0.00 9.26
Dielectric Tensor εij (total)
17.48 0.00 0.00
0.00 17.48 0.00
0.00 0.00 17.48
Polycrystalline dielectric constant εpoly
(electronic contribution)
9.26
Polycrystalline dielectric constant εpoly
(total)
17.48
Refractive Index n
3.04
Potentially ferroelectric?
True

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
60
U Values
--
Pseudopotentials
VASP PAW: Li_sv Na_pv Sb
Final Energy/Atom
-2.8905 eV
Corrected Energy
-11.5621 eV
-11.5621 eV = -11.5621 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 57410
  • 54244

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)