Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.183 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.315 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCo3(BO3)2 + B2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 89.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 208.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 199.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 322.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 148.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 119.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 199.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 259.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 299.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 188.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 208.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 239.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 259.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 89.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 219.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 259.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 219.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 339.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 99.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 339.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 159.3 |
Te2W (mp-22693) | <1 0 1> | <0 1 1> | 199.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 280.1 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 119.5 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 79.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 259.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 323.6 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 323.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 322.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 219.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 159.8 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 323.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 219.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 224.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 300.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 257.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 259.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 323.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 345.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 199.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 89.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 199.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 199.7 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 199.1 |
CdS (mp-672) | <1 1 1> | <1 1 -1> | 258.9 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 199.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 159.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 219.7 |
YVO4 (mp-19133) | <0 0 1> | <0 1 -1> | 157.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 238.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2B2O5 (mp-18256) | 0.0744 | 0.000 | 3 |
Mg2B2O5 (mp-5547) | 0.0824 | 0.000 | 3 |
Cd2B2O5 (mp-7210) | 0.4654 | 0.000 | 3 |
Mg2B2O5 (mp-560772) | 0.0834 | 0.002 | 3 |
Fe2B2O5 (mp-19333) | 0.2166 | 0.000 | 3 |
LiMn2(CO4)2 (mp-762184) | 0.4370 | 0.071 | 4 |
LiV2(CO4)2 (mp-763553) | 0.4368 | 0.136 | 4 |
LiV(CO3)2 (mp-763116) | 0.4490 | 0.078 | 4 |
LiMn2(CO4)2 (mp-762985) | 0.4344 | 0.072 | 4 |
Li2V(CO3)2 (mp-765106) | 0.4149 | 0.095 | 4 |
RbLi2Cr2(BO3)3 (mp-770630) | 0.7463 | 0.216 | 5 |
Na3MgC2ClO6 (mp-23653) | 0.7059 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Co B O |
Final Energy/Atom-7.1319 eV |
Corrected Energy-141.7962 eV
Uncorrected energy = -128.3742 eV
Composition-based energy adjustment (-0.687 eV/atom x 10.0 atoms) = -6.8700 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -141.7962 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)