Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.041 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.347 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPuGa3 + Ga |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 132.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 184.8 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 328.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 328.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 290.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 79.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 52.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 316.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 132.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 237.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 105.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 328.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 105.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 237.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 263.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 237.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 343.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 290.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 316.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 301.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 184.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 52.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 290.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 301.1 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 237.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 184.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 369.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 343.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 211.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 263.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 132.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 184.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 237.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 132.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 184.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 184.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 211.2 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 65.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 290.4 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 104.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 290.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 211.2 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 263.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 211.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 237.6 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 263.0 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 197.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 263.0 |
BN (mp-984) | <1 0 0> | <0 1 1> | 197.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc5(In2Rh)2 (mp-18645) | 0.7102 | 0.000 | 3 |
Ti4Ga3Ni2 (mp-30705) | 0.7473 | 0.052 | 3 |
Mn3Al9Si (mp-15819) | 0.6503 | 0.000 | 3 |
UAl4 (mp-574122) | 0.2465 | 0.047 | 2 |
PuGa4 (mp-510173) | 0.2095 | 0.347 | 2 |
NpAl4 (mp-16520) | 0.2766 | 0.156 | 2 |
NpGa4 (mp-1080762) | 0.2340 | 0.123 | 2 |
PuAl4 (mp-542776) | 0.4040 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pu Ga_d |
Final Energy/Atom-5.2354 eV |
Corrected Energy-52.3539 eV
-52.3539 eV = -52.3539 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)