Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.507 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcm [57] |
Hall-P 2c 2b |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypePlane
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 277.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 236.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 94.6 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 283.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 97.1 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 71.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 283.7 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 285.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 339.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 242.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 242.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 236.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 156.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 313.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 157.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 313.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 261.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 339.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 242.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 209.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 261.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 339.9 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 236.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 291.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 242.8 |
BN (mp-984) | <1 0 0> | <0 1 1> | 285.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 94.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 242.8 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 242.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 261.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 339.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 277.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 277.7 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 261.5 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 71.4 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 156.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 339.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 0> | 94.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 97.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 52.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 194.3 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 285.5 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 194.3 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 214.1 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 285.5 |
LaF3 (mp-905) | <1 1 0> | <0 1 1> | 285.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 145.7 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 156.9 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 313.8 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 1> | 214.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5SbS (mp-767407) | 0.5734 | 0.094 | 3 |
Ta2V4Si5 (mp-17806) | 0.6390 | 0.180 | 3 |
Mn2Nb9Ge8 (mp-567194) | 0.6170 | 0.121 | 3 |
Mn4Nb7Ge8 (mp-29906) | 0.6423 | 0.141 | 3 |
Nb2V4Si5 (mp-17210) | 0.6488 | 0.184 | 3 |
NiSn (mp-680646) | 0.5766 | 0.008 | 2 |
Ga2Ir (mp-31253) | 0.5992 | 0.000 | 2 |
Re4Si7 (mp-568595) | 0.5804 | 0.000 | 2 |
ThTl (mp-542382) | 0.2577 | 0.000 | 2 |
ZrCu (mp-1080022) | 0.5049 | 0.022 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv Ga_d |
Final Energy/Atom-6.9993 eV |
Corrected Energy-167.9843 eV
Uncorrected energy = -167.9843 eV
Corrected energy = -167.9843 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)