material

In5Se5Br

ID:

mp-510346

DOI:

10.17188/1262892


Tags: Pentaindium pentaselenide bromide

Material Details

Final Magnetic Moment
0.007 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.526 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.025 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
InBr2 + InSe + In2Se3
Band Gap
0.916 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmn21 [31]
Hall
P 2ac 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 414218 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <1 1 1> <0 1 0> 0.000 325.6
Al2O3 (mp-1143) <0 0 1> <0 1 0> 0.005 260.5
SiC (mp-11714) <1 1 0> <0 1 0> 0.010 325.6
MoSe2 (mp-1634) <1 0 1> <0 1 0> 0.015 260.5
AlN (mp-661) <1 1 0> <0 1 0> 0.016 325.6
Au (mp-81) <1 1 0> <0 1 0> 0.019 195.4
GaTe (mp-542812) <1 0 -1> <0 1 1> 0.019 76.3
GaN (mp-804) <1 1 0> <0 1 0> 0.019 260.5
CdS (mp-672) <1 0 1> <0 1 0> 0.023 65.1
Mg (mp-153) <1 0 0> <0 0 1> 0.025 198.8
GaTe (mp-542812) <0 0 1> <0 1 1> 0.027 76.3
LaF3 (mp-905) <0 0 1> <0 0 1> 0.028 318.1
BN (mp-984) <1 0 0> <0 1 0> 0.030 195.4
AlN (mp-661) <1 0 1> <0 0 1> 0.033 357.9
Te2W (mp-22693) <0 1 0> <1 1 0> 0.033 162.2
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.033 357.9
InP (mp-20351) <1 1 1> <0 1 1> 0.034 305.2
InP (mp-20351) <1 0 0> <0 0 1> 0.037 318.1
GaTe (mp-542812) <1 0 1> <0 1 0> 0.039 195.4
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.040 159.1
LiAlO2 (mp-3427) <0 0 1> <1 1 0> 0.040 162.2
Mg (mp-153) <1 1 0> <0 1 0> 0.043 260.5
MoSe2 (mp-1634) <1 0 0> <0 1 0> 0.046 260.5
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.048 153.7
TiO2 (mp-390) <0 0 1> <0 0 1> 0.050 278.4
WS2 (mp-224) <1 0 1> <0 0 1> 0.050 278.4
Mg (mp-153) <0 0 1> <0 0 1> 0.050 278.4
BN (mp-984) <0 0 1> <0 0 1> 0.057 357.9
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.060 119.3
Te2W (mp-22693) <1 0 0> <0 1 0> 0.061 195.4
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.071 278.4
InSb (mp-20012) <1 1 1> <1 0 1> 0.077 153.7
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.079 325.6
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.079 278.4
WS2 (mp-224) <0 0 1> <0 0 1> 0.080 278.4
ZrO2 (mp-2858) <1 1 -1> <0 1 1> 0.082 228.9
Ga2O3 (mp-886) <1 0 -1> <0 1 0> 0.083 195.4
ZnO (mp-2133) <1 0 0> <0 1 0> 0.083 260.5
CdTe (mp-406) <1 1 1> <1 0 1> 0.085 153.7
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.086 278.4
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 0.088 153.7
ZnO (mp-2133) <1 0 1> <0 1 0> 0.091 195.4
AlN (mp-661) <0 0 1> <0 0 1> 0.095 318.1
BaTiO3 (mp-5986) <1 0 1> <0 1 0> 0.095 325.6
GaTe (mp-542812) <1 0 0> <0 1 1> 0.099 228.9
GaN (mp-804) <1 0 0> <0 0 1> 0.101 198.8
WSe2 (mp-1821) <1 0 1> <0 1 0> 0.104 260.5
InSb (mp-20012) <1 0 0> <0 0 1> 0.105 357.9
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.108 357.9
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.109 318.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
51 20 16 0 0 0
20 32 19 0 0 0
16 19 59 0 0 0
0 0 0 19 0 0
0 0 0 0 13 0
0 0 0 0 0 12
Compliance Tensor Sij (10-12Pa-1)
26.5 -15.3 -2.1 0 0 0
-15.3 48.3 -11.7 0 0 0
-2.1 -11.7 21.4 0 0 0
0 0 0 53.9 0 0
0 0 0 0 78.8 0
0 0 0 0 0 80
Shear Modulus GV
14 GPa
Bulk Modulus KV
28 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
26 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
27 GPa
Elastic Anisotropy
0.56
Poisson's Ratio
0.28

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.00000 0.31357
-0.59157 -0.74010 -0.30921 0.00000 0.00000 0.00000
0.00000 0.00000 0.00000 -0.09403 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.99665 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
11.09 0.00 0.00
0.00 10.36 0.00
0.00 0.00 10.18
Dielectric Tensor εij (total)
37.39 0.00 0.00
0.00 28.12 0.00
0.00 0.00 34.18
Polycrystalline dielectric constant εpoly
(electronic contribution)
10.54
Polycrystalline dielectric constant εpoly
(total)
33.23
Refractive Index n
3.25
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
In5S5Cl (mp-31263) 0.4342 0.000 3
In5Se5Cl (mp-568603) 0.4722 0.024 3
Yb3(Sb7Te12)2 (mp-675683) 0.5974 0.099 3
In5S5Br (mp-510347) 0.2585 0.000 3
In10(Pb2S7)3 (mp-662823) 0.6078 0.002 3
Mg2NiWO6 (mvc-5066) 0.6760 0.192 4
Cu4Bi5PbS11 (mp-672295) 0.6440 0.027 4
Li9Ti7Nb5O30 (mp-767497) 0.6323 0.050 4
Li8Ti6Mn7O30 (mp-773922) 0.6314 0.084 4
Li8Ti7Nb6O30 (mp-772997) 0.6411 0.079 4
Cr5S8 (mp-849084) 0.7304 0.223 2
LiCa3Zr3TaO12 (mp-677136) 0.7443 0.004 5
Cu6AgBi12PbS22 (mp-651706) 0.6996 0.025 5
La7SmTi3V5O20 (mp-1076885) 0.7460 0.274 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d Se Br
Final Energy/Atom
-3.5150 eV
Corrected Energy
-83.1180 eV
Uncorrected energy = -77.3300 eV Composition-based energy adjustment (-0.534 eV/atom x 2.0 atoms) = -1.0680 eV Composition-based energy adjustment (-0.472 eV/atom x 10.0 atoms) = -4.7200 eV Corrected energy = -83.1180 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 414218
Submitted by
User remarks:
  • Pentaindium pentaselenide bromide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)