material

TiSiNi

ID:

mp-510409

DOI:

10.17188/1262916


Tags: Nickel titanium silicide (1/1/1) Titanium nickel silicide (1/1/1) Titanium nickel silicon (1/1/1) - E-phase

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.847 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.64 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 0 0> <1 1 1> 0.007 331.3
Mg (mp-153) <1 1 0> <0 1 0> 0.026 231.8
SiC (mp-8062) <1 1 0> <0 0 1> 0.029 135.4
TiO2 (mp-2657) <1 0 1> <0 1 1> 0.030 102.7
Te2W (mp-22693) <0 1 0> <1 0 0> 0.032 216.6
Ag (mp-124) <1 0 0> <1 1 1> 0.050 331.3
SiC (mp-11714) <1 0 1> <1 0 0> 0.061 130.0
Ge (mp-32) <1 1 1> <1 0 0> 0.067 173.3
CdTe (mp-406) <1 1 1> <1 0 0> 0.076 303.2
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.080 293.3
InSb (mp-20012) <1 1 1> <1 0 0> 0.087 303.2
GaTe (mp-542812) <0 0 1> <0 0 1> 0.107 225.7
GaAs (mp-2534) <1 1 1> <1 0 0> 0.107 173.3
Bi2Se3 (mp-541837) <0 0 1> <0 1 1> 0.108 137.0
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.109 270.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.112 135.4
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.112 203.1
LaF3 (mp-905) <0 0 1> <0 1 1> 0.115 137.0
KCl (mp-23193) <1 1 0> <0 1 0> 0.119 231.8
SiC (mp-7631) <1 0 1> <1 1 1> 0.126 331.3
C (mp-48) <1 1 1> <0 1 0> 0.133 334.8
LaF3 (mp-905) <1 0 0> <0 0 1> 0.134 270.8
WS2 (mp-224) <0 0 1> <0 1 0> 0.135 283.3
MoS2 (mp-1434) <0 0 1> <0 1 0> 0.136 283.3
Te2W (mp-22693) <0 1 1> <0 1 0> 0.136 231.8
CdWO4 (mp-19387) <1 1 1> <0 1 0> 0.138 51.5
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.149 173.3
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.155 248.2
PbSe (mp-2201) <1 1 0> <1 0 0> 0.160 216.6
CdS (mp-672) <0 0 1> <0 1 1> 0.163 137.0
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.176 225.7
Ni (mp-23) <1 1 0> <0 0 1> 0.177 158.0
Mg (mp-153) <0 0 1> <0 1 0> 0.177 283.3
GaN (mp-804) <1 1 0> <0 1 0> 0.181 231.8
GaP (mp-2490) <1 1 0> <0 0 1> 0.182 338.5
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.182 97.7
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.183 146.5
TePb (mp-19717) <1 0 0> <0 1 1> 0.185 171.2
KP(HO2)2 (mp-23959) <0 0 1> <1 1 0> 0.197 151.2
MoSe2 (mp-1634) <0 0 1> <0 1 1> 0.205 171.2
WSe2 (mp-1821) <0 0 1> <0 1 1> 0.206 171.2
LaAlO3 (mp-2920) <0 0 1> <0 1 1> 0.222 102.7
TePb (mp-19717) <1 1 1> <1 0 0> 0.226 303.2
C (mp-48) <1 0 1> <0 0 1> 0.227 180.5
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.230 231.8
TbScO3 (mp-31119) <1 0 0> <1 1 1> 0.233 276.1
InAs (mp-20305) <1 0 0> <0 0 1> 0.238 112.8
GaN (mp-804) <1 0 1> <0 0 1> 0.241 135.4
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.241 171.2
Cu (mp-30) <1 1 0> <0 0 1> 0.246 112.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
287 98 124 0 0 0
98 326 130 0 0 0
124 130 274 0 0 0
0 0 0 114 0 0
0 0 0 0 129 0
0 0 0 0 0 108
Compliance Tensor Sij (10-12Pa-1)
4.4 -0.7 -1.7 0 0 0
-0.7 3.9 -1.5 0 0 0
-1.7 -1.5 5.1 0 0 0
0 0 0 8.8 0 0
0 0 0 0 7.7 0
0 0 0 0 0 9.3
Shear Modulus GV
106 GPa
Bulk Modulus KV
177 GPa
Shear Modulus GR
102 GPa
Bulk Modulus KR
176 GPa
Shear Modulus GVRH
104 GPa
Bulk Modulus KVRH
177 GPa
Elastic Anisotropy
0.19
Poisson's Ratio
0.25

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
12
U Values
--
Pseudopotentials
VASP PAW: Ni_pv Si Ti_pv
Final Energy/Atom
-7.2140 eV
Corrected Energy
-86.5676 eV
-86.5676 eV = -86.5676 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 646619
  • 18188
  • 165253

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)