Final Magnetic Moment2.918 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.721 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAgRuO4 + Ag2O + RuO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4122 [91] |
HallP 4w 2c |
Point Group422 |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 184.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 244.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 266.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 244.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 160.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 307.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 266.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 307.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 213.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 266.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 244.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 266.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 307.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 266.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 213.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 245.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 61.5 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 260.8 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 244.1 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 162.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 266.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 307.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 266.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 213.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 307.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 244.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 173.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 61.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 213.3 |
Al (mp-134) | <1 1 1> | <1 0 0> | 245.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 53.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 184.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 213.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 260.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 266.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 184.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 213.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 160.0 |
BN (mp-984) | <1 0 1> | <1 1 0> | 260.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 184.4 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 307.3 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 244.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 260.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 86.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 184.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 213.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 184.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 266.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 266.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd4Ni3O10 (mp-567184) | 0.6253 | 0.053 | 3 |
Ag3IrO4 (mp-776370) | 0.3196 | 0.071 | 3 |
Sb2WO6 (mp-541435) | 0.6235 | 0.000 | 3 |
Ba3Y2Br12 (mp-777292) | 0.6517 | 0.067 | 3 |
Ba3(YI6)2 (mp-776579) | 0.5522 | 0.078 | 3 |
Mg2SnWO6 (mvc-5015) | 0.6070 | 0.156 | 4 |
LiLa4Ti3O12 (mp-756861) | 0.6479 | 0.031 | 4 |
Li5Cu3(TeO5)2 (mp-755495) | 0.6247 | 0.106 | 4 |
CaLaMn2O6 (mp-25765) | 0.6836 | 0.109 | 4 |
AlNi(WO4)2 (mvc-613) | 0.6838 | 0.231 | 4 |
Ca14La6Mg3Ti17O60 (mp-695227) | 0.6486 | 0.011 | 5 |
Ca3La5Mn6(CuO12)2 (mp-706245) | 0.6684 | 0.150 | 5 |
Ca2La2MgTi3O12 (mp-676461) | 0.6696 | 0.032 | 5 |
Li3La8Ti9Cr3O36 (mp-743640) | 0.6557 | 0.066 | 5 |
Ca10La6Mg3Ti13O48 (mp-695254) | 0.6750 | 0.014 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Ru_pv O |
Final Energy/Atom-5.0657 eV |
Corrected Energy-173.3375 eV
-173.3375 eV = -162.1008 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)