Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.933 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Cr2O3 + SiO2 |
Band Gap3.139 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 201.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 291.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 186.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 194.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 201.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 162.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 339.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 186.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 339.7 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 339.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 139.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 244.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 244.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 194.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 201.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 244.1 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 269.0 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 225.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 232.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 232.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 162.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 225.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 339.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 194.1 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 225.8 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 254.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 339.7 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 269.0 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 244.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 93.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 169.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 232.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 194.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 339.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 244.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 339.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 242.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 244.1 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 269.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 291.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 203.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 242.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 232.9 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 326.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 97.1 |
BN (mp-984) | <1 0 1> | <0 1 1> | 201.8 |
BN (mp-984) | <1 1 1> | <0 0 1> | 139.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 339.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 339.7 |
Al (mp-134) | <1 1 1> | <0 1 0> | 339.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.3709 | 0.012 | 3 |
MnSiO3 (mp-19528) | 0.4924 | 0.003 | 3 |
MgSiO3 (mp-1020125) | 0.4268 | 0.009 | 3 |
MgSiO3 (mp-1020361) | 0.3109 | 0.009 | 3 |
MgSiO3 (mp-1020117) | 0.3789 | 0.009 | 3 |
LiV(SiO3)2 (mp-640515) | 0.1114 | 0.000 | 4 |
LiSc(SiO3)2 (mp-6099) | 0.2919 | 0.001 | 4 |
LiFe(SiO3)2 (mp-19061) | 0.1712 | 0.001 | 4 |
MgSi2WO6 (mvc-6890) | 0.3786 | 0.332 | 4 |
LiGa(SiO3)2 (mp-6241) | 0.1950 | 0.041 | 4 |
NaLi7Fe8(SiO3)16 (mp-775490) | 0.5233 | 0.003 | 5 |
Li7Cr3Co(PO4)6 (mp-780115) | 0.5428 | 0.073 | 5 |
Li8Mg3Cu9(SiO3)16 (mp-774516) | 0.5439 | 0.064 | 5 |
Li7Fe3Ni(PO4)6 (mp-775193) | 0.5316 | 0.047 | 5 |
Li2MgCu2(SiO3)4 (mp-773087) | 0.5438 | 0.053 | 5 |
Li2MnVP2(O4F)2 (mp-777226) | 0.6524 | 0.022 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6565 | 0.073 | 6 |
Li4TiCo2Ni3(PO4)6 (mp-778251) | 0.6438 | 0.085 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.6385 | 0.100 | 6 |
Li2MnVP2(O4F)2 (mp-776709) | 0.6572 | 0.020 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6681 | 0.002 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7173 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv O Si Cr_pv |
Final Energy/Atom-7.5111 eV |
Corrected Energy-325.3495 eV