Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.544 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Group3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 63.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 90.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 254.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 127.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 318.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 63.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 63.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 110.3 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 110.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 318.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 318.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 180.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 90.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 63.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 318.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 90.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 90.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 318.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 318.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 254.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 254.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 180.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 318.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 270.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 191.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 191.0 |
BN (mp-984) | <1 0 1> | <1 1 0> | 180.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 318.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 318.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 318.3 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 180.1 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 270.1 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 270.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 191.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 318.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 318.3 |
C (mp-66) | <1 0 0> | <1 0 0> | 63.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 90.0 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 90.0 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 63.7 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 318.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 254.6 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 318.3 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 318.3 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 318.3 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 90.0 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 90.0 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 63.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 318.3 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 180.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsEuCl3 (mp-1068377) | 0.1016 | 0.007 | 3 |
LiUO3 (mp-545712) | 0.0984 | 0.208 | 3 |
Fe(NF2)3 (mp-1079464) | 0.0455 | 1.329 | 3 |
Al(NF2)3 (mp-1079140) | 0.0519 | 1.832 | 3 |
BaBiO3 (mp-23438) | 0.0253 | 0.025 | 3 |
Rb2NaTlF6 (mp-989548) | 0.0240 | 0.000 | 4 |
Rb2NaSbF6 (mp-989541) | 0.0239 | 0.000 | 4 |
Sr2MgIrO6 (mp-16307) | 0.0241 | 0.000 | 4 |
Ba2DyBiO6 (mp-545659) | 0.0241 | 0.000 | 4 |
Ba2YBiO6 (mp-23137) | 0.0240 | 0.000 | 4 |
Ca3Sb2 (mp-1013546) | 0.1134 | 0.421 | 2 |
Ba3Sb2 (mp-1013582) | 0.1134 | 0.409 | 2 |
Ca3Bi2 (mp-1013735) | 0.1134 | 0.366 | 2 |
Sr3Sb2 (mp-1013583) | 0.1134 | 0.381 | 2 |
Ni4N (mp-20839) | 0.1134 | 2.021 | 2 |
BaCaLaBiO6 (mp-39886) | 0.0304 | 0.155 | 5 |
BaLaTaZnO6 (mp-42054) | 0.0242 | 0.120 | 5 |
BaLaMgTaO6 (mp-40251) | 0.0423 | 0.080 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0519 | 0.126 | 5 |
BaLaMnMoO6 (mp-622596) | 0.0541 | 0.189 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7260 | 0.065 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eVMo: 4.38 eV |
PseudopotentialsVASP PAW: Sr_sv Co Mo_pv O |
Final Energy/Atom-6.6843 eV |
Corrected Energy-152.9230 eV
-152.9230 eV = -133.6855 eV (uncorrected energy) - 10.8100 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|