Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.919 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGaPO4 + Ni3(PO4)2 + PH6NO4 + Ni3N + H2O + N2 |
Band Gap4.132 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 1> | 187.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 275.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 139.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 139.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 275.9 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 275.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 275.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 139.5 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 275.9 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 139.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 275.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 275.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 275.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 92.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 139.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 187.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 275.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 275.9 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 275.9 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 187.1 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 139.5 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 275.9 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 275.9 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 275.9 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 275.9 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 275.9 |
C (mp-48) | <0 0 1> | <1 1 0> | 147.5 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 275.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 275.9 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 92.0 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 275.9 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 230.6 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 275.9 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 275.9 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 275.9 |
MgF2 (mp-1249) | <1 1 1> | <1 1 -1> | 180.9 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 92.0 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 183.9 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 92.0 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 275.9 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 275.9 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 187.1 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 137.0 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 183.9 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 275.9 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 275.9 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 92.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMo3P3O16 (mp-25083) | 0.7374 | 0.010 | 4 |
Li2Cr2H4O9 (mp-743649) | 0.5569 | 0.009 | 4 |
Mn3Ga4P6(H2O5)6 (mp-762167) | 0.4141 | 0.018 | 5 |
KAl2P2H5O11 (mp-730945) | 0.5436 | 0.007 | 5 |
KAl2P2H4O11 (mp-758536) | 0.6433 | 0.102 | 5 |
V8Sn16H85(C8O9)4 (mp-705959) | 0.7356 | 0.283 | 5 |
KAl2NiP3(H2O7)2 (mp-744988) | 0.4803 | 0.100 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ga_d Ni_pv P H N O |
Final Energy/Atom-6.0303 eV |
Corrected Energy-373.7466 eV
-373.7466 eV = -349.7545 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)