Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.837 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 279.0 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 241.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 167.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 241.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 204.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 254.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 260.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 254.1 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 148.6 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 99.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 334.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 297.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 203.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 274.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 203.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 148.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 93.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 186.0 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 137.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 229.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 353.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 260.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 203.3 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 297.6 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 216.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 229.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 321.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 198.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 254.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 223.2 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 148.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 334.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 321.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 223.2 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 274.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 45.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 204.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 99.1 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 297.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 49.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 49.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 93.0 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 55.8 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 130.2 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 260.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 316.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 241.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 274.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 216.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 183.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.3739 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.4687 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.4414 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.3856 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.7001 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.4614 | 0.106 | 4 |
NdGe (mp-663) | 0.0379 | 0.000 | 2 |
ScSi (mp-9969) | 0.0974 | 0.000 | 2 |
SmGe (mp-972521) | 0.0956 | 0.000 | 2 |
TmSi (mp-1066975) | 0.1287 | 0.000 | 2 |
LuSi (mp-1001612) | 0.1192 | 0.000 | 2 |
Si (mp-1001113) | 0.6978 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Ge_d |
Final Energy/Atom-5.5363 eV |
Corrected Energy-22.1450 eV
-22.1450 eV = -22.1450 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)