Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-2.442 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/n [85] |
HallP 4ab 1ab |
Point Group4/m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 84.3 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 309.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 233.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 184.0 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 278.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 327.1 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 218.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 233.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 84.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 119.2 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 218.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 218.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 218.0 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 281.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 112.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 337.3 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 357.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 233.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 278.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 233.5 |
BN (mp-984) | <1 0 1> | <1 0 0> | 140.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 196.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 168.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 238.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 186.8 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 218.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 309.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 218.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 119.2 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 252.9 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 0 0> | 252.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 196.7 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 306.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 318.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 281.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 218.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 357.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 168.6 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 218.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 84.3 |
Al (mp-134) | <1 1 0> | <1 1 0> | 119.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 140.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 318.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 318.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 224.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 184.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 281.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 218.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 159.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 238.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SiMoP3O11 (mp-585483) | 0.7002 | 0.000 | 4 |
SiP3RuO11 (mp-562501) | 0.6408 | 0.027 | 4 |
Mn7Co(PO4)12 (mp-762148) | 0.7140 | 0.081 | 4 |
ZrFe(PO4)3 (mp-769438) | 0.6714 | 0.084 | 4 |
Mn7Fe(PO4)12 (mp-778021) | 0.7085 | 0.074 | 4 |
Cr5O12 (mp-773920) | 0.7156 | 0.000 | 2 |
LiBiF5 (mp-752483) | 0.4631 | 0.064 | 3 |
RePO5 (mp-867296) | 0.6161 | 0.000 | 3 |
SiP2O7 (mp-1020608) | 0.5041 | 0.086 | 3 |
CoP2O7 (mp-31529) | 0.5993 | 0.092 | 3 |
Al2(SeO4)3 (mp-780398) | 0.6000 | 0.026 | 3 |
YbK2Sn(PO4)3 (mp-677714) | 0.7110 | 0.022 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points12 |
U Values-- |
PseudopotentialsVASP PAW: B F Ag |
Final Energy/Atom-4.8156 eV |
Corrected Energy-67.4184 eV
-67.4184 eV = -67.4184 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)