material

Ca(AsPd)2

ID:

mp-5166

DOI:

10.17188/1263119


Tags: High pressure experimental phase Calcium palladium arsenide (1/2/2) Calcium dipalladium arsenide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.744 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 36372 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <1 1 1> <0 0 1> 0.001 95.2
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.001 152.4
CaCO3 (mp-3953) <1 1 1> <0 0 1> 0.005 152.4
InAs (mp-20305) <1 0 0> <0 0 1> 0.005 38.1
SiC (mp-11714) <0 0 1> <1 1 1> 0.007 66.1
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.008 247.6
Te2Mo (mp-602) <1 1 0> <1 1 0> 0.009 189.9
SiC (mp-7631) <0 0 1> <1 1 1> 0.009 66.1
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.010 38.1
GaP (mp-2490) <1 0 0> <0 0 1> 0.014 152.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.016 209.5
SiC (mp-7631) <1 0 1> <1 1 0> 0.016 189.9
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.017 247.6
TePb (mp-19717) <1 0 0> <0 0 1> 0.021 171.4
ZrO2 (mp-2858) <0 1 0> <1 0 1> 0.021 194.6
LiGaO2 (mp-5854) <0 0 1> <1 0 0> 0.027 223.8
SiC (mp-8062) <1 0 0> <0 0 1> 0.028 19.0
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.031 152.4
Mg (mp-153) <1 1 1> <0 0 1> 0.034 152.4
Cu (mp-30) <1 0 0> <0 0 1> 0.036 171.4
Te2Mo (mp-602) <1 0 0> <1 1 1> 0.042 330.5
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.054 171.4
SiC (mp-8062) <1 1 1> <0 0 1> 0.054 361.9
GaN (mp-804) <1 1 1> <0 0 1> 0.055 152.4
BN (mp-984) <1 1 0> <0 0 1> 0.060 133.3
Au (mp-81) <1 1 0> <1 0 0> 0.069 223.8
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.091 323.8
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.091 152.4
CdSe (mp-2691) <1 0 0> <0 0 1> 0.097 38.1
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.100 253.2
ZnO (mp-2133) <1 0 0> <1 1 0> 0.103 189.9
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.103 323.8
SiC (mp-11714) <1 0 0> <1 1 0> 0.103 63.3
MgF2 (mp-1249) <1 1 1> <1 0 1> 0.104 243.2
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.116 243.2
SiC (mp-7631) <1 0 0> <0 0 1> 0.121 95.2
LiF (mp-1138) <1 0 0> <0 0 1> 0.123 152.4
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.126 316.5
GaSb (mp-1156) <1 0 0> <0 0 1> 0.129 38.1
ZnO (mp-2133) <0 0 1> <1 0 1> 0.140 194.6
LaF3 (mp-905) <0 0 1> <0 0 1> 0.145 228.5
Ni (mp-23) <1 1 0> <1 0 1> 0.147 243.2
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.147 228.5
Ga2O3 (mp-886) <1 0 -1> <1 1 1> 0.152 264.4
Ag (mp-124) <1 1 0> <1 0 0> 0.153 223.8
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.154 268.5
SiO2 (mp-6930) <1 1 1> <1 1 1> 0.157 264.4
BN (mp-984) <0 0 1> <0 0 1> 0.163 133.3
GaN (mp-804) <1 0 1> <1 1 1> 0.163 132.2
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.163 152.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
132 47 74 0 0 0
47 132 74 0 0 0
74 74 137 0 0 0
0 0 0 28 0 0
0 0 0 0 28 0
0 0 0 0 0 15
Compliance Tensor Sij (10-12Pa-1)
11 -0.8 -5.5 0 0 0
-0.8 11 -5.5 0 0 0
-5.5 -5.5 13.2 0 0 0
0 0 0 35.3 0 0
0 0 0 0 35.3 0
0 0 0 0 0 66.3
Shear Modulus GV
28 GPa
Bulk Modulus KV
88 GPa
Shear Modulus GR
25 GPa
Bulk Modulus KR
86 GPa
Shear Modulus GVRH
27 GPa
Bulk Modulus KVRH
87 GPa
Elastic Anisotropy
0.61
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sm(GePd)2 (mp-31491) 0.0158 0.000 3
Pr(SiPt)2 (mp-567338) 0.0289 0.000 3
Nd(SiPt)2 (mp-20950) 0.0281 0.076 3
Nd(GePd)2 (mp-4725) 0.0270 0.000 3
Eu(SiPt)2 (mp-1076931) 0.0256 0.000 3
La3Cu4(P2O)2 (mp-6309) 0.6709 0.000 4
EuGa4 (mp-21884) 0.1551 0.000 2
ThZn4 (mp-536) 0.1277 0.000 2
SrGa4 (mp-1827) 0.1716 0.000 2
BaIn4 (mp-22687) 0.1954 0.000 2
BaGa4 (mp-335) 0.0054 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv As Pd
Final Energy/Atom
-5.0780 eV
Corrected Energy
-25.3902 eV
Uncorrected energy = -25.3902 eV Corrected energy = -25.3902 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 36372
  • 188177
  • 188178
  • 604341
  • 190703
Submitted by
User remarks:
  • Calcium dipalladium arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)