material

RbAlF4

ID:

mp-5259

DOI:

10.17188/1263167


Tags: Rubidium tetrafluoroluminate Rubidium tetrafluoroaluminate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.658 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
< 0.001 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
RbAlF4
Band Gap
6.944 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/mbm [127]
Hall
-P 4 2ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 54120 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-66) <1 0 0> <0 0 1> 0.001 217.6
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.004 244.8
GaTe (mp-542812) <0 0 1> <1 0 1> 0.006 301.6
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.007 108.8
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.007 244.8
WS2 (mp-224) <0 0 1> <1 1 0> 0.008 141.8
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.008 141.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.008 27.2
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.013 43.1
GaN (mp-804) <1 0 0> <1 0 0> 0.017 33.4
Mg (mp-153) <1 1 0> <1 0 1> 0.019 86.2
GaP (mp-2490) <1 0 0> <0 0 1> 0.020 244.8
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.020 167.1
CsI (mp-614603) <1 0 0> <0 0 1> 0.022 244.8
Mg (mp-153) <0 0 1> <1 1 0> 0.024 141.8
CdTe (mp-406) <1 0 0> <0 0 1> 0.024 217.6
Mg (mp-153) <1 0 0> <1 0 0> 0.024 33.4
PbS (mp-21276) <1 1 1> <1 1 0> 0.024 189.1
LiAlO2 (mp-3427) <1 1 1> <1 1 1> 0.027 54.5
LiGaO2 (mp-5854) <1 0 1> <1 1 1> 0.028 272.7
MoSe2 (mp-1634) <1 0 1> <1 0 1> 0.028 258.5
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.028 190.4
GaTe (mp-542812) <1 0 -1> <1 0 1> 0.029 301.6
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.029 190.4
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.030 217.6
InSb (mp-20012) <1 0 0> <0 0 1> 0.030 217.6
TiO2 (mp-390) <1 0 1> <1 0 0> 0.035 200.6
AlN (mp-661) <1 0 0> <1 0 1> 0.036 172.4
GaN (mp-804) <0 0 1> <1 1 0> 0.037 141.8
KCl (mp-23193) <1 1 0> <1 0 0> 0.037 234.0
Mg (mp-153) <1 1 1> <0 0 1> 0.039 244.8
Al2O3 (mp-1143) <1 1 0> <1 0 1> 0.039 215.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.039 217.6
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.039 108.8
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.042 244.8
LiTaO3 (mp-3666) <1 0 0> <1 0 1> 0.043 215.5
Te2W (mp-22693) <0 0 1> <1 0 0> 0.045 66.9
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.054 27.2
Te2W (mp-22693) <0 1 1> <1 0 1> 0.054 172.4
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.055 33.4
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.055 190.4
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.056 47.3
Al (mp-134) <1 1 0> <1 0 0> 0.056 234.0
MoSe2 (mp-1634) <1 0 0> <1 0 1> 0.057 258.5
GaN (mp-804) <1 1 0> <1 0 1> 0.059 86.2
ZrO2 (mp-2858) <1 0 1> <1 0 1> 0.063 43.1
Ni (mp-23) <1 1 1> <1 1 0> 0.064 189.1
C (mp-48) <1 0 0> <1 0 1> 0.064 215.5
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.065 190.4
AlN (mp-661) <1 1 0> <1 1 0> 0.067 330.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
87 21 21 0 0 0
21 87 21 0 0 0
21 21 78 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 63
Compliance Tensor Sij (10-12Pa-1)
12.8 -2.3 -2.8 0 0 0
-2.3 12.8 -2.8 0 0 0
-2.8 -2.8 14.3 0 0 0
0 0 0 58 0 0
0 0 0 0 58 0
0 0 0 0 0 15.9
Shear Modulus GV
32 GPa
Bulk Modulus KV
42 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
42 GPa
Shear Modulus GVRH
29 GPa
Bulk Modulus KVRH
42 GPa
Elastic Anisotropy
1.28
Poisson's Ratio
0.22

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
2.05 0.00 0.00
0.00 2.05 0.00
0.00 0.00 2.02
Dielectric Tensor εij (total)
7.32 0.00 0.00
0.00 7.32 0.00
0.00 0.00 7.17
Polycrystalline dielectric constant εpoly
(electronic contribution)
2.04
Polycrystalline dielectric constant εpoly
(total)
7.27
Refractive Index n
1.43
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AlTlF4 (mp-5606) 0.5390 0.002 3
KAlF4 (mp-2910) 0.3132 0.013 3
RbAlF4 (mp-5479) 0.5524 0.001 3
AlTlF4 (mp-557233) 0.1962 0.001 3
RbAlF4 (mp-4693) 0.3739 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Rb_sv Al F
Final Energy/Atom
-5.3925 eV
Corrected Energy
-64.7104 eV
-64.7104 eV = -64.7104 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 200638
  • 54121
  • 54120
Submitted by
User remarks:
  • Rubidium tetrafluoroluminate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)