Final Magnetic Moment1.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.503 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 210.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 150.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 187.9 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 187.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 152.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 152.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 187.9 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 0> | 150.0 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 152.4 |
TiO2 (mp-2657) | <1 0 0> | <1 -1 0> | 180.7 |
C (mp-66) | <1 0 0> | <0 1 0> | 152.4 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 152.4 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 152.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 210.0 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 -1> | 167.6 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 1 0> | 152.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 152.4 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 187.9 |
Fe2O3 (mp-24972) | <1 0 1> | <1 0 0> | 150.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb4CrS8 (mp-5306) | 0.5677 | 0.006 | 3 |
Ta4AgS8 (mp-677597) | 0.5600 | 0.000 | 3 |
Ta4MnS8 (mp-3581) | 0.5827 | 0.039 | 3 |
Mn(NbS2)4 (mp-3669) | 0.5656 | 0.022 | 3 |
Nb4CoS8 (mp-1094100) | 0.6125 | 0.000 | 3 |
LiV2O2F3 (mp-765853) | 0.7411 | 0.066 | 4 |
LiMn2O2F3 (mp-767005) | 0.6991 | 0.040 | 4 |
LiFe2O2F3 (mp-774121) | 0.7227 | 0.068 | 4 |
ZnCuBiO5 (mvc-8909) | 0.7490 | 0.131 | 4 |
Ti7S12 (mp-673657) | 0.6543 | 0.000 | 2 |
Ti13S24 (mp-684731) | 0.6214 | 0.002 | 2 |
Nb25S48 (mp-684620) | 0.1565 | 0.000 | 2 |
V5S8 (mp-690772) | 0.7364 | 0.000 | 2 |
Nb3S5 (mp-32983) | 0.3497 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv S |
Final Energy/Atom-7.9156 eV |
Corrected Energy-642.6752 eV
-642.6752 eV = -609.5022 eV (uncorrected energy) - 33.1730 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)