Final Magnetic Moment0.110 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.438 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTb5S7 + Tb2S3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21212 [18] |
HallP 2 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 278.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 208.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 278.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 197.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 278.3 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 197.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 139.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 278.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 278.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 139.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 197.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 208.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 139.1 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 197.7 |
C (mp-66) | <1 1 0> | <1 1 0> | 197.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 278.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 208.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 278.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 278.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 69.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 197.7 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 156.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 208.7 |
Au (mp-81) | <1 1 0> | <1 1 0> | 197.7 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 278.3 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 278.3 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 278.3 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 278.3 |
GaTe (mp-542812) | <0 0 1> | <0 1 1> | 155.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 69.6 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 278.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 278.3 |
Si (mp-149) | <1 0 0> | <0 0 1> | 278.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 69.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 139.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 278.3 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 197.7 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 69.6 |
GaTe (mp-542812) | <1 0 -1> | <0 1 1> | 155.8 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 139.1 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 278.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nd10US16 (mp-685926) | 0.2012 | 0.028 | 3 |
Pr10US16 (mp-675336) | 0.2313 | 0.028 | 3 |
Ce10US16 (mp-676880) | 0.2468 | 0.018 | 3 |
La10US16 (mp-675741) | 0.2859 | 0.033 | 3 |
Tb14(PbSe8)3 (mp-676110) | 0.3191 | 0.043 | 3 |
Er2S3 (mp-684708) | 0.1606 | 0.041 | 2 |
Ho2S3 (mp-32787) | 0.1530 | 0.035 | 2 |
Dy2S3 (mp-32826) | 0.1553 | 0.025 | 2 |
Y2S3 (mp-32891) | 0.1561 | 0.036 | 2 |
Dy11S16 (mp-531574) | 0.0334 | 0.032 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 S |
Final Energy/Atom-6.3845 eV |
Corrected Energy-365.9933 eV
-365.9933 eV = -344.7626 eV (uncorrected energy) - 21.2307 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)