Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.428 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr3S4 + Nb3S5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 155.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 194.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 269.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 194.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 271.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 271.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 194.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 349.3 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 269.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 232.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 271.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 116.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 242.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 194.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 271.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 349.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 155.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 271.7 |
Ag (mp-124) | <1 1 0> | <1 1 1> | 145.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 116.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 271.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 194.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 194.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 116.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 38.8 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 116.4 |
BN (mp-984) | <0 0 1> | <1 0 1> | 269.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 271.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 310.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 310.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 271.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 140.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 116.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 271.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 310.5 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 242.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 271.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 116.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 194.0 |
Al (mp-134) | <1 1 0> | <1 1 0> | 140.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 116.4 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 242.7 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 310.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 310.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 194.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 140.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 155.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 271.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ta4MnS8 (mp-3581) | 0.2733 | 0.039 | 3 |
Ta4FeS8 (mp-554416) | 0.2113 | 0.000 | 3 |
Mn(NbS2)4 (mp-3669) | 0.1773 | 0.022 | 3 |
Nb4CoS8 (mp-1094100) | 0.1765 | 0.000 | 3 |
Mn(NbS2)4 (mp-675257) | 0.2542 | 0.022 | 3 |
LiCo3OF5 (mp-764144) | 0.7420 | 0.129 | 4 |
LiMnOF2 (mp-766798) | 0.7401 | 0.078 | 4 |
LiCoOF2 (mp-850916) | 0.7297 | 0.301 | 4 |
LiMn2O2F3 (mp-767005) | 0.6780 | 0.040 | 4 |
Li2Co(WO4)2 (mp-556321) | 0.7390 | 0.000 | 4 |
Cr5S8 (mp-849084) | 0.5600 | 0.223 | 2 |
Ti7S12 (mp-673657) | 0.6249 | 0.000 | 2 |
Ta27S50 (mp-530018) | 0.5677 | 0.000 | 2 |
V5S8 (mp-690772) | 0.5357 | 0.000 | 2 |
Nb3S5 (mp-32983) | 0.3746 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Cr_pv S |
Final Energy/Atom-7.4161 eV |
Corrected Energy-200.8669 eV
Uncorrected energy = -192.8189 eV
Composition-based energy adjustment (-0.503 eV/atom x 16.0 atoms) = -8.0480 eV
Corrected energy = -200.8669 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)