Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.698 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.971 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 144.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 240.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 240.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 153.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 240.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 337.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 337.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 240.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 288.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 337.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 153.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 153.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 240.7 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 144.4 |
SiC (mp-7631) | <1 1 1> | <0 1 1> | 160.5 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 153.1 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 96.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 337.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 337.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 240.7 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 144.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 192.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 288.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 337.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 240.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 144.4 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 337.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 240.7 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 144.4 |
SiC (mp-11714) | <1 1 0> | <0 1 1> | 160.5 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 337.0 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 337.0 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 337.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 288.8 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 337.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 192.5 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 337.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 192.5 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 144.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 144.4 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 337.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 240.7 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 288.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 288.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 144.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 337.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 153.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.4 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 144.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 288.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2PdO3 (mp-760483) | 0.0949 | 0.000 | 3 |
Li2SnO3 (mp-3540) | 0.0784 | 0.000 | 3 |
Li2MoO3 (mp-35975) | 0.1192 | 0.000 | 3 |
Li2RhO3 (mp-754870) | 0.1036 | 0.000 | 3 |
Li2IrO3 (mp-532085) | 0.1037 | 0.000 | 3 |
Li4Cr3NiO8 (mp-769999) | 0.1378 | 0.052 | 4 |
Li4Cr3FeO8 (mp-770303) | 0.1349 | 0.585 | 4 |
Li4Cr3NiO8 (mp-770039) | 0.1269 | 0.072 | 4 |
Li3Fe(NiO3)2 (mp-773709) | 0.1031 | 0.013 | 4 |
Li3V2FeO6 (mp-771840) | 0.1255 | 0.014 | 4 |
LiTe3 (mp-27466) | 0.2840 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.2551 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2779 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.2664 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2251 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5919 | 0.005 | 5 |
Hg (mp-982872) | 0.3688 | 0.020 | 1 |
Sb (mp-632286) | 0.4261 | 0.059 | 1 |
Se (mp-7755) | 0.4306 | 0.181 | 1 |
Te (mp-10654) | 0.3972 | 0.047 | 1 |
Te (mp-105) | 0.3370 | 0.047 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Pt O |
Final Energy/Atom-5.4689 eV |
Corrected Energy-419.0438 eV
-419.0438 eV = -393.7613 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)