Final Magnetic Moment0.014 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.653 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCuO + Al2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 287.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 230.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 230.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 136.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 172.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 287.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 154.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 136.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 287.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 57.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 230.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 136.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 57.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 172.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 287.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 57.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 115.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 115.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 172.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 115.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 230.3 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 140.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 287.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 57.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 140.8 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 154.8 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 154.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 287.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 57.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 287.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 172.7 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 172.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 172.7 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 136.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 115.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 287.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 287.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 115.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 172.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 57.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 287.8 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 136.3 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 1> | 154.8 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 230.3 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 136.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 -1> | 140.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2CuO4 (mp-530977) | 0.0810 | 0.057 | 3 |
Al2CuO4 (mp-531283) | 0.1035 | 0.062 | 3 |
MgAl2O4 (mp-531340) | 0.1004 | 0.031 | 3 |
Al2CuO4 (mp-34728) | 0.1088 | 0.059 | 3 |
Al2CuO4 (mvc-16141) | 0.1069 | 0.059 | 3 |
Li5Fe7O3F13 (mp-851009) | 0.1499 | 0.053 | 4 |
Li2V3CoO8 (mp-774950) | 0.1537 | 0.145 | 4 |
Li3MgV8O16 (mp-771733) | 0.1404 | 0.023 | 4 |
Li2V3FeO8 (mp-776146) | 0.1542 | 0.030 | 4 |
Li3Zn(Fe5O8)4 (mp-771780) | 0.1639 | 0.067 | 4 |
Fe3O4 (mp-715491) | 0.2760 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.2730 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.2410 | 0.057 | 2 |
Fe3O4 (mp-715558) | 0.2839 | 0.076 | 2 |
Fe3O4 (mp-715811) | 0.2878 | 0.076 | 2 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2209 | 0.029 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.1926 | 0.019 | 5 |
Li4Al3Cr3(SbO8)2 (mp-770625) | 0.2213 | 0.003 | 5 |
Li4Nb3V3(SnO8)2 (mp-767976) | 0.2131 | 0.098 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.2049 | 0.053 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6711 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6770 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6843 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6804 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6825 | 0.661 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al Cu_pv O |
Final Energy/Atom-6.7346 eV |
Corrected Energy-499.5157 eV
-499.5157 eV = -471.4241 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)