material

B13N2

ID:

mp-534

DOI:

10.17188/1263490


Tags: Boron nitride (13/2)

Material Details

Final Magnetic Moment
1.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.254 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.135 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BN + B
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 162801 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 1 1> <0 0 1> 0.001 339.5
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.010 182.8
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.010 182.8
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.017 182.8
LaF3 (mp-905) <0 0 1> <0 0 1> 0.018 182.8
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.020 339.5
BN (mp-984) <0 0 1> <0 0 1> 0.024 104.5
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.029 204.5
GdScO3 (mp-5690) <0 1 1> <1 0 0> 0.038 272.6
Mg (mp-153) <0 0 1> <0 0 1> 0.053 26.1
InP (mp-20351) <1 1 1> <0 0 1> 0.055 182.8
WS2 (mp-224) <1 1 1> <0 0 1> 0.059 78.3
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.077 136.3
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.079 204.5
TbScO3 (mp-31119) <0 1 1> <1 0 0> 0.080 272.6
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.086 156.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.103 235.0
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.109 156.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.113 235.0
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.120 136.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.121 26.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.122 26.1
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.127 52.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.147 287.3
LaF3 (mp-905) <1 1 1> <1 0 0> 0.154 204.5
Mg (mp-153) <1 1 0> <1 0 1> 0.164 146.0
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.165 182.8
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.172 272.6
SiO2 (mp-6930) <1 0 0> <1 0 0> 0.177 136.3
InSb (mp-20012) <1 1 0> <0 0 1> 0.211 313.4
CdTe (mp-406) <1 1 0> <0 0 1> 0.224 313.4
GaP (mp-2490) <1 0 0> <0 0 1> 0.235 208.9
GaTe (mp-542812) <1 0 0> <1 0 0> 0.237 136.3
Mg (mp-153) <1 1 1> <0 0 1> 0.244 208.9
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.277 208.9
AlN (mp-661) <1 0 0> <1 0 0> 0.279 204.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.281 104.5
AlN (mp-661) <1 1 0> <1 0 0> 0.287 136.3
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.292 208.9
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.294 313.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.296 78.3
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.299 156.7
Si (mp-149) <1 1 0> <0 0 1> 0.301 208.9
LaF3 (mp-905) <1 1 0> <1 0 0> 0.302 272.6
LiF (mp-1138) <1 1 1> <0 0 1> 0.321 339.5
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.322 78.3
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.330 208.9
Te2W (mp-22693) <0 0 1> <1 1 1> 0.331 241.8
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.344 156.7
ZrO2 (mp-2858) <1 0 0> <1 0 1> 0.357 146.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
521 136 83 49 0 0
136 521 83 -49 0 0
83 83 541 0 0 0
49 -49 0 123 0 0
0 0 0 0 123 49
0 0 0 0 49 193
Compliance Tensor Sij (10-12Pa-1)
2.2 -0.6 -0.2 -1.1 0 0
-0.6 2.2 -0.2 1.1 0 0
-0.2 -0.2 1.9 0 0 0
-1.1 1.1 0 9 0 0
0 0 0 0 9 -2.3
0 0 0 0 -2.3 5.8
Shear Modulus GV
173 GPa
Bulk Modulus KV
243 GPa
Shear Modulus GR
148 GPa
Bulk Modulus KR
243 GPa
Shear Modulus GVRH
161 GPa
Bulk Modulus KVRH
243 GPa
Elastic Anisotropy
0.86
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiB13C2 (mp-638070) 0.6579 0.000 3
LiB13C2 (mp-655591) 0.6526 0.012 3
B4C (mp-696746) 0.2302 0.071 2
B13C2 (mp-576) 0.2932 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: B N
Final Energy/Atom
-7.1064 eV
Corrected Energy
-107.3182 eV
Uncorrected energy = -106.5962 eV Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV Corrected energy = -107.3182 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 162801
Submitted by
User remarks:
  • Boron nitride (13/2)