Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.515 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6/mmm [191] |
Hall-P 6 2 |
Point Group6/mmm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 287.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 210.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 287.6 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 235.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 195.6 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 168.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 149.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 234.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 286.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 287.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 225.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 278.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 171.1 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 105.3 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 338.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 165.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 135.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 106.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 234.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 278.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 64.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 150.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 60.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 208.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 213.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 156.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 165.5 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 287.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 225.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 52.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 286.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 165.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 300.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 270.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 134.8 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 209.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 195.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 130.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 331.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 255.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 165.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 195.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 269.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points35 |
U Values-- |
PseudopotentialsVASP PAW: B Co Er_3 |
Final Energy/Atom-7.0579 eV |
Corrected Energy-42.3475 eV
-42.3475 eV = -42.3475 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)