Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.763 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 130.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 184.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 184.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 130.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 130.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 184.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 130.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 184.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 261.1 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 184.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 130.5 |
Al (mp-134) | <1 1 0> | <1 1 0> | 184.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 184.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 130.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 184.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 130.5 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 261.1 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 184.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 184.6 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 130.5 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 184.6 |
MgAl2O4 (mp-3536) | <1 0 0> | <1 0 0> | 130.5 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 184.6 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 130.5 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 130.5 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 184.6 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 184.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 130.5 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 184.6 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 261.1 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 130.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 130.5 |
MgF2 (mp-1249) | <1 1 0> | <1 1 0> | 184.6 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 261.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zr6Si7Ni16 (mp-570166) | 0.0612 | 0.000 | 3 |
Mg6Ni16Ge7 (mp-21725) | 0.0863 | 0.000 | 3 |
Zr6Ni16Ge7 (mp-672651) | 0.0455 | 0.000 | 3 |
Zr6Co16Si7 (mp-672680) | 0.0981 | 0.000 | 3 |
Sc6Ni16Ge7 (mp-570547) | 0.0297 | 0.000 | 3 |
Yb6Fe23 (mp-669649) | 0.3636 | 0.073 | 2 |
Zr6Co23 (mp-30569) | 0.3553 | 0.000 | 2 |
Zr6Fe23 (mp-582924) | 0.2344 | 0.000 | 2 |
Er6Zn23 (mp-30615) | 0.2452 | 0.010 | 2 |
Sr6Mg23 (mp-30782) | 0.3665 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv Si Ni_pv |
Final Energy/Atom-6.5708 eV |
Corrected Energy-190.5524 eV
Uncorrected energy = -190.5524 eV
Corrected energy = -190.5524 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)