Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.508 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMo(PO4)2 |
Band Gap2.492 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 141.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 153.7 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 247.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 247.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 322.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 322.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 322.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 257.8 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 172.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 204.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 164.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 257.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 256.2 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 164.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 257.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 193.3 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 172.6 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 164.7 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 172.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 153.7 |
BN (mp-984) | <1 0 0> | <0 1 0> | 153.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 141.8 |
Al (mp-134) | <1 1 0> | <0 1 1> | 164.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 257.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 257.8 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 307.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 172.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 141.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 193.3 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 172.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 322.2 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 136.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 204.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 193.3 |
C (mp-66) | <1 1 0> | <0 1 0> | 307.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 322.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 322.2 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 247.0 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 172.6 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 150.8 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 204.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 204.9 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 256.2 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 256.2 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 -1> | 136.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 204.9 |
Au (mp-81) | <1 0 0> | <1 0 1> | 172.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 193.3 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 141.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-771363) | 0.4757 | 0.025 | 3 |
Hg2P2O7 (mp-28455) | 0.4276 | 0.000 | 3 |
Co2P3O10 (mp-25658) | 0.4722 | 0.020 | 3 |
Mn2P3O10 (mp-31981) | 0.4468 | 0.030 | 3 |
Cr2P3O10 (mp-31635) | 0.4340 | 0.057 | 3 |
Li7Cr2P7O24 (mp-773702) | 0.4115 | 0.071 | 4 |
LiFe(PO3)3 (mp-699324) | 0.4020 | 0.032 | 4 |
LiFe(PO3)3 (mp-540313) | 0.3672 | 0.032 | 4 |
LiMn2P3O11 (mp-540021) | 0.3705 | 0.041 | 4 |
LiCo(PO3)3 (mp-540275) | 0.4226 | 0.025 | 4 |
MnFeCo(PO4)3 (mp-764410) | 0.5247 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.5254 | 0.029 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.5195 | 0.044 | 5 |
NaZnFe2(PO4)3 (mp-566178) | 0.4938 | 0.007 | 5 |
SrVZnP2O9 (mp-555402) | 0.5266 | 0.007 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6975 | 0.081 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6920 | 0.255 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6415 | 0.015 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.7023 | 0.100 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6791 | 0.081 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Li_sv Mo_pv P O |
Final Energy/Atom-7.0088 eV |
Corrected Energy-373.0198 eV
-373.0198 eV = -336.4225 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 14.1240 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)