Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.358 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.217 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + LiPO3 |
Band Gap1.617 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 349.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 306.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 349.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 349.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 218.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 218.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 174.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 218.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 131.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 306.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 87.5 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 221.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 87.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 153.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 262.4 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 221.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 349.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 43.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 76.7 |
BN (mp-984) | <1 0 1> | <1 1 1> | 161.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 221.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 349.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 294.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 -1> | 146.5 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 221.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 230.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 221.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 174.9 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 -1> | 221.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 76.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 87.5 |
C (mp-66) | <1 1 1> | <1 0 0> | 43.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 174.9 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 218.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 -1> | 221.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 221.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 218.7 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 174.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 87.5 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 43.7 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 221.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 306.7 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 1> | 201.5 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 349.8 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 87.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 153.3 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 153.3 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 230.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 230.0 |
Au (mp-81) | <1 1 1> | <1 0 0> | 87.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.24934 | 0.16192 | 0.09786 | 0.00000 | 0.09243 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.04589 | 0.00000 | -0.09974 |
0.02390 | -0.04010 | -0.11406 | 0.00000 | -0.12976 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.33676 C/m2 |
Crystallographic Direction vmax |
---|
-3.00000 |
-1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.59 | 0.00 | 0.03 |
0.00 | 2.84 | 0.00 |
0.03 | 0.00 | 3.18 |
Dielectric Tensor εij (total) |
||
---|---|---|
4.11 | 0.00 | 0.21 |
0.00 | 5.77 | 0.00 |
0.21 | 0.00 | 7.76 |
Polycrystalline dielectric constant
εpoly∞
2.87
|
Polycrystalline dielectric constant
εpoly
5.88
|
Refractive Index n1.69 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe(Si2O3)2 (mp-744274) | 0.6243 | 0.996 | 3 |
Cr4(PO4)3 (mp-504357) | 0.7171 | 0.784 | 3 |
Li2Cr2O7 (mp-769775) | 0.6307 | 0.039 | 3 |
P2Pd2O7 (mp-554320) | 0.6756 | 0.013 | 3 |
Cu5(Si2O7)2 (mp-25205) | 0.7182 | 0.115 | 3 |
LiFeP2O7 (mp-694534) | 0.1258 | 0.263 | 4 |
LiCrP2O7 (mp-696040) | 0.1416 | 0.236 | 4 |
LiCrP2O7 (mp-540482) | 0.0958 | 0.236 | 4 |
LiMnP2O7 (mp-694614) | 0.1108 | 0.217 | 4 |
LiNiP2O7 (mp-540164) | 0.1312 | 0.136 | 4 |
Cs2Li2B2P4O15 (mp-1019606) | 0.6912 | 0.000 | 5 |
LiCu2P3(HO5)2 (mp-849424) | 0.7272 | 0.071 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8974 eV |
Corrected Energy-164.9375 eV
-164.9375 eV = -151.7437 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)