Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.403 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.172 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + LiPO3 |
Band Gap1.304 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 251.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 224.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 224.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 311.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 230.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 112.2 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 311.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 230.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 312.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 230.7 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 256.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 186.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 251.4 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 307.7 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 224.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 336.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 224.4 |
BN (mp-984) | <0 0 1> | <1 1 0> | 299.7 |
BN (mp-984) | <1 0 1> | <1 0 1> | 224.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 224.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 311.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 224.4 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 153.8 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 230.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 307.7 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 230.7 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 230.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 299.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 224.4 |
CdTe (mp-406) | <1 1 1> | <1 0 1> | 224.4 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 224.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 224.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 156.3 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 311.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 230.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 112.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 230.7 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 224.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 168.3 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 230.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 199.8 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 311.2 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 224.4 |
TiO2 (mp-2657) | <0 0 1> | <1 1 -1> | 197.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 224.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 311.2 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 251.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 280.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 -1> | 230.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 224.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr6P7O24 (mp-504359) | 0.4893 | 0.021 | 3 |
Ge2BiO6 (mvc-8139) | 0.4772 | 0.111 | 3 |
Hg2P2O7 (mp-28455) | 0.4304 | 0.000 | 3 |
Mn2P3O10 (mp-31981) | 0.4132 | 0.030 | 3 |
Cr2P3O10 (mp-31635) | 0.4484 | 0.057 | 3 |
ZnNiP2O7 (mvc-5701) | 0.3118 | 0.019 | 4 |
MgNiP2O7 (mvc-5642) | 0.3608 | 0.026 | 4 |
VZnP2O7 (mvc-5556) | 0.2527 | 0.047 | 4 |
LiNiP2O7 (mp-32321) | 0.3526 | 0.103 | 4 |
LiCoP2O7 (mp-540375) | 0.3099 | 0.082 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.4234 | 0.087 | 5 |
KNaZnP2O7 (mp-554157) | 0.5791 | 0.000 | 5 |
Na2ZrNi(P2O7)2 (mp-18984) | 0.5839 | 0.058 | 5 |
NaLiMnP2O7 (mp-778279) | 0.5432 | 0.203 | 5 |
SrVZnP2O9 (mp-555402) | 0.5565 | 0.007 | 5 |
LiMnVP2(HO5)2 (mp-765378) | 0.7068 | 0.046 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.7178 | 0.257 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.7168 | 0.075 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6762 | 0.072 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.7051 | 0.725 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5865 | 0.068 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7278 | 0.071 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.9424 eV |
Corrected Energy-331.8550 eV
-331.8550 eV = -305.4675 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)