Final Magnetic Moment0.290 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.111 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.209 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiPO4 |
Band Gap0.261 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 163.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 170.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 163.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 170.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 170.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 170.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 170.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 163.4 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 163.4 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 170.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 170.5 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 163.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 170.5 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 170.5 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 163.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Be(GaO2)2 (mp-676950) | 0.4131 | 0.116 | 3 |
Zn2SiO4 (mp-1020721) | 0.4602 | 0.111 | 3 |
Zn2SiO4 (mp-1020636) | 0.3634 | 0.052 | 3 |
Li2SO4 (mp-4556) | 0.4024 | 0.000 | 3 |
Li2BeF4 (mp-4622) | 0.4438 | 0.000 | 3 |
LiCrPO4 (mp-775710) | 0.2179 | 0.524 | 4 |
LiCrPO4 (mp-773799) | 0.2140 | 0.067 | 4 |
LiNiPO4 (mp-705448) | 0.1921 | 0.223 | 4 |
Li3Cu(PO4)2 (mp-504348) | 0.2134 | 0.064 | 4 |
LiFePO4 (mp-585433) | 0.1915 | 0.795 | 4 |
Ge3N4 (mp-672289) | 0.6822 | 0.000 | 2 |
Si3N4 (mp-2245) | 0.6829 | 0.000 | 2 |
SiC2 (mp-1019097) | 0.6118 | 0.562 | 2 |
CN2 (mp-1077595) | 0.6555 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.6597 | 0.118 | 2 |
YAl6Si18(N15O)2 (mp-677127) | 0.6163 | 0.092 | 5 |
NdAl6Si30(N15O)3 (mp-532626) | 0.6525 | 0.067 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.6669 | 0.000 | 5 |
LiAl3Si9(N7O)2 (mp-695365) | 0.6017 | 0.046 | 5 |
YAl6Si30(N15O)3 (mp-677140) | 0.6256 | 0.084 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.6791 | 0.003 | 6 |
C (mp-568410) | 0.6281 | 0.507 | 1 |
C (mp-1008374) | 0.7165 | 0.437 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.1002 eV |
Corrected Energy-767.8416 eV
Uncorrected energy = -683.2176 eV
Composition-based energy adjustment (-0.687 eV/atom x 64.0 atoms) = -43.9680 eV
Composition-based energy adjustment (-2.541 eV/atom x 16.0 atoms) = -40.6560 eV
Corrected energy = -767.8416 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)