Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.403 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.143 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + Fe2O3 + Li3PO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 219.3 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 288.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 204.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 288.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 141.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 336.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 192.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 141.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 288.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 204.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 240.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 144.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 48.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 102.1 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 141.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 288.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 336.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 240.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 102.1 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.7 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 141.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 336.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 336.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 288.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 336.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 141.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 204.3 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 240.1 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 240.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 240.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 240.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 240.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 141.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 225.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 240.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 204.3 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 219.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 192.1 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 288.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 225.7 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 288.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 192.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 336.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 102.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 144.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 141.4 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 336.2 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 336.2 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 240.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 225.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2SiO4 (mp-675299) | 0.6557 | 0.105 | 3 |
La2Fe2O5 (mp-1099626) | 0.6818 | 0.072 | 3 |
Ca2Fe2O5 (mp-25750) | 0.6529 | 0.000 | 3 |
Ca3Al2O6 (mp-12147) | 0.6539 | 0.013 | 3 |
La2Mn2O5 (mp-1099627) | 0.6527 | 0.095 | 3 |
Ca2AlSnO5 (mvc-5761) | 0.5615 | 0.146 | 4 |
Na4TiAs2O9 (mp-559519) | 0.4855 | 0.000 | 4 |
Li4MnP2O9 (mp-761599) | 0.1858 | 0.019 | 4 |
Li4MoP2O9 (mp-540075) | 0.2959 | 0.068 | 4 |
Li4CrP2O9 (mp-540457) | 0.2129 | 0.039 | 4 |
Li2CrPO4F (mp-770894) | 0.6107 | 0.151 | 5 |
Li5MnP2(O4F)2 (mp-762699) | 0.6202 | 0.036 | 5 |
Li5VP2(O4F)2 (mp-568287) | 0.5457 | 0.052 | 5 |
La7SmMn6(FeO10)2 (mp-1076797) | 0.6200 | 0.131 | 5 |
La6Sm2Cr3(FeO4)5 (mp-1099892) | 0.6230 | 0.169 | 5 |
Li3VCrP2(HO5)2 (mp-767626) | 0.7340 | 0.068 | 6 |
Li4Mn2Fe3P6WO24 (mp-770860) | 0.7285 | 0.174 | 6 |
Li4Fe2Ni3Sn(PO4)6 (mp-781476) | 0.7258 | 0.081 | 6 |
Li4TiCu2Ni3(PO4)6 (mp-776613) | 0.7373 | 0.101 | 6 |
Li4Co2Ni3Sn(PO4)6 (mp-776757) | 0.7406 | 0.139 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.3034 eV |
Corrected Energy-219.8157 eV
-219.8157 eV = -201.7085 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)