Final Magnetic Moment0.019 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.383 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToErNi + Er |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 249.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 62.3 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 132.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 186.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 311.4 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 146.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 62.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 249.1 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 146.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 311.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 186.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 311.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 249.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 249.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 186.9 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 0> | 264.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 311.4 |
Au (mp-81) | <1 1 0> | <1 0 1> | 146.3 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 62.3 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 249.1 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 0> | 264.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 62.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 264.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 249.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 311.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 311.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 311.4 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 311.4 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 186.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 311.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 132.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 132.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 186.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 264.7 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 186.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 311.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 62.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 62.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 62.3 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 264.7 |
MoSe2 (mp-1634) | <1 1 1> | <1 0 0> | 264.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 311.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 132.4 |
C (mp-48) | <1 1 1> | <1 0 0> | 132.4 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 249.1 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 249.1 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 249.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 186.9 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 311.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 311.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(YbGe)4 (mp-646071) | 0.6832 | 0.032 | 3 |
Pr2Sc3Si4 (mp-568831) | 0.6384 | 0.000 | 3 |
Tb2Ti3Si4 (mp-510083) | 0.6806 | 0.000 | 3 |
Sc2Re3Si4 (mp-16794) | 0.6216 | 0.000 | 3 |
Ce2Sc3Si4 (mp-505512) | 0.6187 | 0.000 | 3 |
Sm3Rh2 (mp-17391) | 0.5252 | 0.000 | 2 |
Sr3Ag2 (mp-30357) | 0.1877 | 0.000 | 2 |
Sr3Au2 (mp-30421) | 0.4033 | 0.000 | 2 |
Ba3Ag2 (mp-12612) | 0.4170 | 0.000 | 2 |
Zr5Si4 (mp-1304) | 0.5495 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Ni_pv |
Final Energy/Atom-5.4356 eV |
Corrected Energy-81.5347 eV
-81.5347 eV = -81.5347 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)