Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.233 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGeSe2 |
Band Gap1.438 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 278.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 278.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 278.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 92.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 248.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 155.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 92.9 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 278.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 278.6 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 278.6 |
ZnO (mp-2133) | <1 0 0> | <0 1 0> | 278.6 |
SrTiO3 (mp-4651) | <1 1 1> | <0 1 0> | 278.6 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 0> | 92.9 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 0> | 278.6 |
Al2O3 (mp-1143) | <1 0 0> | <0 1 0> | 185.7 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 278.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 278.6 |
C (mp-66) | <1 0 0> | <0 1 0> | 278.6 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 278.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 155.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 155.1 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 92.9 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 278.6 |
LaF3 (mp-905) | <1 1 0> | <0 1 0> | 92.9 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 278.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 185.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 278.6 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 278.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 278.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbBS3 (mp-9047) | 0.4565 | 0.000 | 3 |
TlBS3 (mp-28809) | 0.3592 | 0.007 | 3 |
Tl2B2Se7 (mp-16183) | 0.4730 | 0.000 | 3 |
K2B2S7 (mp-4351) | 0.4640 | 0.000 | 3 |
GaPS4 (mp-30979) | 0.3436 | 0.000 | 3 |
K6Cd4Sn3Se13 (mp-6296) | 0.7401 | 0.030 | 4 |
CsAgPSe3 (mp-865980) | 0.5829 | 0.000 | 4 |
TlInSiS4 (mp-556744) | 0.6562 | 0.000 | 4 |
GaAg(PSe3)2 (mp-654129) | 0.6994 | 0.000 | 4 |
GeS2 (mp-542613) | 0.3595 | 0.000 | 2 |
GeS2 (mp-622213) | 0.4754 | 0.049 | 2 |
Ge4Se9 (mp-680333) | 0.3078 | 0.027 | 2 |
GeS2 (mp-572892) | 0.1435 | 0.030 | 2 |
SiS2 (mp-1095294) | 0.5061 | 0.022 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d Se |