Final Magnetic Moment4.810 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.085 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.439 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToWO3 + Eu2WO6 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 258.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 91.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 183.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 134.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 91.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 134.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 91.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 258.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 91.9 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 251.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 134.5 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 186.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 186.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 183.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 275.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 86.1 |
BN (mp-984) | <1 0 0> | <0 1 1> | 251.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 172.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 91.9 |
Al (mp-134) | <1 0 0> | <0 1 0> | 258.4 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 183.7 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 186.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 91.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 183.7 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 183.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 159.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 91.9 |
C (mp-48) | <1 0 1> | <1 1 0> | 159.7 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 91.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 275.6 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 183.7 |
ZnO (mp-2133) | <0 0 1> | <1 0 1> | 186.7 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 186.7 |
SrTiO3 (mp-4651) | <1 1 1> | <0 0 1> | 275.6 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 134.5 |
Ge (mp-32) | <1 1 0> | <1 0 1> | 186.7 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 134.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 275.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 91.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 275.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 183.7 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 183.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 275.6 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 275.6 |
Si (mp-149) | <1 1 1> | <0 1 0> | 258.4 |
Au (mp-81) | <1 0 0> | <0 0 1> | 275.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 172.3 |
C (mp-48) | <1 1 0> | <0 1 0> | 172.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 134.5 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 183.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tb2(WO4)3 (mp-770351) | 0.0871 | 0.036 | 3 |
Ce2(WO4)3 (mp-505428) | 0.1092 | 0.079 | 3 |
Gd2(WO4)3 (mp-773192) | 0.0849 | 0.646 | 3 |
Sm2(WO4)3 (mp-773126) | 0.0883 | 0.024 | 3 |
Nd2(WO4)3 (mp-25188) | 0.0999 | 0.025 | 3 |
EuMoO4F (mp-686947) | 0.6351 | 0.499 | 4 |
BiPPbO5 (mp-556878) | 0.6053 | 0.000 | 4 |
VBiPbO5 (mp-566459) | 0.6640 | 0.000 | 4 |
VBiPbO5 (mp-510666) | 0.6823 | 0.002 | 4 |
ErMoO4F (mp-565302) | 0.6901 | 0.000 | 4 |
SrLaTl(AsO4)2 (mp-685195) | 0.7481 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Eu W_pv O |
Final Energy/Atom-7.8116 eV |
Corrected Energy-308.7104 eV
Uncorrected energy = -265.5944 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-4.438 eV/atom x 6.0 atoms) = -26.6280 eV
Corrected energy = -308.7104 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)