Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.565 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.888 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 234.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 234.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 117.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 150.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 167.8 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 191.0 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 191.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 138.6 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 138.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 234.7 |
Al (mp-134) | <1 1 1> | <1 0 1> | 167.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 147.5 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 191.0 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 150.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 221.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 294.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 294.9 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 1> | 167.8 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 294.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 294.9 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 221.2 |
NdGaO3 (mp-3196) | <1 1 0> | <0 1 0> | 117.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 167.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 117.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 294.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 294.9 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 234.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 234.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 234.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 221.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 294.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 221.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 167.8 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 147.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 0> | 191.0 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 0> | 234.7 |
Si (mp-149) | <1 0 0> | <0 1 0> | 117.4 |
Si (mp-149) | <1 1 0> | <0 0 1> | 294.9 |
C (mp-48) | <1 0 0> | <1 1 0> | 191.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 294.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 294.9 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 147.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 221.2 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 234.7 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 117.4 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 221.2 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 221.2 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 221.2 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 73.7 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 294.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ReO5 (mp-505390) | 0.2113 | 0.000 | 3 |
Rb2FeF5 (mp-555378) | 0.3762 | 0.000 | 3 |
K2FeF5 (mp-565539) | 0.3309 | 0.000 | 3 |
Cs2TlCl5 (mp-541696) | 0.3446 | 0.000 | 3 |
Ba2WO5 (mp-504949) | 0.2249 | 0.000 | 3 |
ReSbOF10 (mp-554432) | 0.6507 | 0.000 | 4 |
Ba4Ti2PtO10 (mp-558894) | 0.7467 | 0.000 | 4 |
K2TiOF4 (mp-556623) | 0.7022 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Dy_3 Cl |
Final Energy/Atom-4.1486 eV |
Corrected Energy-145.0346 eV
Uncorrected energy = -132.7546 eV
Composition-based energy adjustment (-0.614 eV/atom x 20.0 atoms) = -12.2800 eV
Corrected energy = -145.0346 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)