material

TiAlCo2

ID:

mp-5407

DOI:

10.17188/1264732


Tags: Aluminium cobalt titanium (1/2/1) Cobalt titanium aluminium (2/1/1)

Material Details

Final Magnetic Moment
0.999 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.625 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.45 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 606679 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <0 0 1> <1 0 0> 0.000 272.2
Cu (mp-30) <1 0 0> <1 0 0> 0.000 170.1
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.000 306.2
C (mp-66) <1 1 0> <1 1 0> 0.002 144.3
InAs (mp-20305) <1 0 0> <1 0 0> 0.002 306.2
GaP (mp-2490) <1 0 0> <1 0 0> 0.005 272.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.010 306.2
Mg (mp-153) <1 1 1> <1 0 0> 0.012 272.2
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.015 176.8
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.019 136.1
Ni (mp-23) <1 1 0> <1 1 0> 0.023 192.5
Mg (mp-153) <0 0 1> <1 1 1> 0.026 235.7
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.029 272.2
WS2 (mp-224) <1 1 1> <1 1 1> 0.031 235.7
GaN (mp-804) <1 0 0> <1 1 0> 0.038 336.8
AlN (mp-661) <0 0 1> <1 1 1> 0.040 58.9
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.040 272.2
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.043 144.3
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.045 176.8
WS2 (mp-224) <1 1 0> <1 1 1> 0.046 235.7
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.046 306.2
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.051 96.2
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.053 170.1
CdSe (mp-2691) <1 0 0> <1 0 0> 0.055 306.2
CsI (mp-614603) <1 0 0> <1 0 0> 0.057 306.2
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.065 136.1
Ag (mp-124) <1 1 1> <1 0 0> 0.066 238.2
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.082 235.7
WS2 (mp-224) <0 0 1> <1 1 1> 0.083 235.7
GaSb (mp-1156) <1 0 0> <1 0 0> 0.085 306.2
Si (mp-149) <1 0 0> <1 0 0> 0.094 272.2
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.102 272.2
LiGaO2 (mp-5854) <0 1 0> <1 1 1> 0.108 294.6
PbSe (mp-2201) <1 0 0> <1 0 0> 0.131 306.2
BN (mp-984) <0 0 1> <1 1 0> 0.135 192.5
Au (mp-81) <1 1 1> <1 0 0> 0.145 238.2
TePb (mp-19717) <1 0 0> <1 0 0> 0.147 170.1
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.148 136.1
Te2W (mp-22693) <0 1 1> <1 1 0> 0.149 288.7
SiC (mp-8062) <1 1 1> <1 1 1> 0.150 235.7
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.164 272.2
SiC (mp-8062) <1 0 0> <1 0 0> 0.168 170.1
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.169 272.2
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.187 170.1
GaN (mp-804) <1 1 1> <1 0 0> 0.193 272.2
C (mp-48) <1 1 1> <1 1 1> 0.200 235.7
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.217 204.1
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.220 306.2
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.227 96.2
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.229 144.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
261 136 136 0 0 0
136 261 136 0 0 0
136 136 261 0 0 0
0 0 0 115 0 0
0 0 0 0 115 0
0 0 0 0 0 115
Compliance Tensor Sij (10-12Pa-1)
5.9 -2 -2 0 0 0
-2 5.9 -2 0 0 0
-2 -2 5.9 0 0 0
0 0 0 8.7 0 0
0 0 0 0 8.7 0
0 0 0 0 0 8.7
Shear Modulus GV
94 GPa
Bulk Modulus KV
178 GPa
Shear Modulus GR
86 GPa
Bulk Modulus KR
178 GPa
Shear Modulus GVRH
90 GPa
Bulk Modulus KVRH
178 GPa
Elastic Anisotropy
0.45
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiCo2Sn (mp-21467) 0.0000 0.000 3
LiIn2Pt (mp-20265) 0.0000 0.000 3
Cd2AgAu (mp-31170) 0.0000 0.000 3
CrGaFe2 (mp-30570) 0.0000 0.087 3
Li2CdSb (mp-16271) 0.0000 0.035 3
LiMgSnPd (mp-7555) 0.0000 0.000 4
LiMgSnAu (mp-7554) 0.0000 0.058 4
VFeCoGe (mp-1063914) 0.0000 0.000 4
LiMgSbPd (mp-10179) 0.0000 0.090 4
LiMgSnPt (mp-11806) 0.0000 0.000 4
Fe3Si (mp-2199) 0.0000 0.000 2
Ni3Sb (mp-10260) 0.0000 0.044 2
Li3Au (mp-11247) 0.0000 0.000 2
Li3Pd (mp-11489) 0.0000 0.000 2
Cu3Sb (mp-2002) 0.0000 0.163 2
Er (mp-10753) 0.0000 0.143 1
W (mp-91) 0.0000 0.000 1
Tm (mp-10661) 0.0000 0.141 1
Ho (mp-7236) 0.0000 0.145 1
Pb (mp-22692) 0.0000 0.048 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Al Co
Final Energy/Atom
-7.0894 eV
Corrected Energy
-28.3575 eV
Uncorrected energy = -28.3575 eV Corrected energy = -28.3575 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 606682
  • 606680
  • 606685
  • 606679
  • 185966
Submitted by
User remarks:
  • Aluminium cobalt titanium (1/2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)