Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.905 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.312 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 231.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 101.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 231.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 231.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 308.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 308.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 171.9 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 231.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 154.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 101.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 101.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 77.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 231.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 308.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 77.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 308.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 231.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 231.7 |
KP(HO2)2 (mp-23959) | <1 1 1> | <0 1 0> | 154.5 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 154.5 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 308.9 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 154.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 231.7 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 154.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 154.5 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 1> | 255.3 |
Si (mp-149) | <1 0 0> | <0 1 0> | 231.7 |
Si (mp-149) | <1 1 1> | <0 0 1> | 101.6 |
WSe2 (mp-1821) | <1 0 0> | <0 1 0> | 154.5 |
WSe2 (mp-1821) | <1 1 0> | <0 1 1> | 255.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 231.7 |
ZrO2 (mp-2858) | <1 1 1> | <0 1 1> | 255.3 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 1> | 255.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 77.2 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 203.3 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 231.7 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 1> | 127.6 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 231.7 |
TiO2 (mp-390) | <0 0 1> | <0 1 0> | 231.7 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 77.2 |
ZnO (mp-2133) | <1 1 1> | <1 1 0> | 188.4 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 308.9 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 0> | 231.7 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 -1> | 138.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi(PO3)4 (mp-26574) | 0.3694 | 0.041 | 3 |
DyP5O14 (mp-554583) | 0.4266 | 0.000 | 3 |
YP5O14 (mp-556335) | 0.4255 | 0.000 | 3 |
Sb(PO3)4 (mp-26150) | 0.4219 | 0.057 | 3 |
Ce(PO3)4 (mp-1019593) | 0.3942 | 0.000 | 3 |
NaY(PO3)4 (mp-555030) | 0.3139 | 0.010 | 4 |
GdAg(PO3)4 (mp-558152) | 0.2525 | 0.069 | 4 |
LaAg(PO3)4 (mp-558465) | 0.3134 | 0.000 | 4 |
NdAg(PO3)4 (mp-541041) | 0.2565 | 0.000 | 4 |
NaGd(PO3)4 (mp-561131) | 0.3014 | 0.000 | 4 |
GdP4H4NO12 (mp-560412) | 0.6038 | 0.005 | 5 |
RbPrP3HO10 (mp-601292) | 0.5300 | 0.035 | 5 |
CsBaLiP2O7 (mp-1019708) | 0.6853 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ce P O |
Final Energy/Atom-7.3301 eV |
Corrected Energy-561.4787 eV
-561.4787 eV = -527.7688 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)