Final Magnetic Moment1.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.274 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.193 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 199.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 214.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 329.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 197.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 214.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 349.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 337.4 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 240.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 245.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 199.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 214.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 276.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 153.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 214.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 131.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 245.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 263.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 299.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 299.5 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 234.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 349.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 329.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 349.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 214.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 240.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 349.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 276.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 175.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 329.3 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 245.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 276.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 349.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 92.0 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 349.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 299.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 65.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 -1> | 312.4 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 276.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 337.4 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 349.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 276.1 |
BN (mp-984) | <1 1 0> | <1 1 0> | 165.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 153.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 153.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 249.6 |
BN (mp-984) | <1 1 1> | <1 1 0> | 165.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 250.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HfTiO4 (mp-753197) | 0.4449 | 0.035 | 3 |
V5Fe3O16 (mp-690125) | 0.4290 | 0.056 | 3 |
Zr5Ti7O24 (mp-860957) | 0.4244 | 0.040 | 3 |
ZrTiO4 (mp-753891) | 0.3910 | 0.044 | 3 |
ZrTi2O6 (mp-757504) | 0.4429 | 0.047 | 3 |
TmCu(WO4)2 (mp-505161) | 0.1654 | 0.035 | 4 |
ErCu(WO4)2 (mp-505167) | 0.1537 | 0.035 | 4 |
HoCu(WO4)2 (mp-556266) | 0.1444 | 0.035 | 4 |
YNi(WO4)2 (mvc-680) | 0.1720 | 0.131 | 4 |
YCu(WO4)2 (mvc-16327) | 0.1817 | 0.033 | 4 |
Pb2O3 (mp-20078) | 0.5726 | 0.009 | 2 |
CrF2 (mp-554340) | 0.6119 | 0.000 | 2 |
V7O13 (mp-556332) | 0.6162 | 0.038 | 2 |
CuF2 (mp-1229) | 0.6034 | 0.000 | 2 |
V7O13 (mp-623373) | 0.6101 | 0.038 | 2 |
Li4NbTe2WO12 (mp-763988) | 0.6713 | 0.075 | 5 |
CaCo2Te3(ClO4)2 (mp-646538) | 0.6611 | 0.068 | 5 |
LaZnFeCuO6 (mvc-9037) | 0.6775 | 0.292 | 5 |
LaTaZnCrO6 (mvc-9887) | 0.6033 | 0.267 | 5 |
LaZnCrCoO6 (mvc-9866) | 0.6747 | 0.361 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Yb_2 Cu_pv W_pv O |
Final Energy/Atom-7.0087 eV |
Corrected Energy-196.8505 eV
-196.8505 eV = -168.2098 eV (uncorrected energy) - 17.4040 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)