Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.560 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.583 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 1> | 126.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 245.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 251.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 289.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 251.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 200.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 251.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 200.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 251.1 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 192.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 251.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 150.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 288.1 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 289.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 247.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 251.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 288.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 50.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 251.1 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 96.6 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 116.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 245.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 200.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 150.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 150.6 |
Al (mp-134) | <1 1 1> | <0 1 0> | 251.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 251.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 288.1 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 192.0 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 1> | 116.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 50.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 251.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 251.1 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 253.4 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 251.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 150.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 150.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 247.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 251.1 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 251.1 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 251.1 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 301.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 247.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 50.2 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 192.0 |
PbSe (mp-2201) | <1 0 0> | <1 1 0> | 192.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 251.1 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 1> | 116.3 |
NdGaO3 (mp-3196) | <1 1 0> | <0 1 0> | 251.1 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 200.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K10Co4O9 (mp-690511) | 0.6742 | 0.000 | 3 |
Cs6Fe2O5 (mp-541385) | 0.4809 | 0.000 | 3 |
Na3CoO3 (mp-774087) | 0.7379 | 0.213 | 3 |
K6Co2O5 (mp-542551) | 0.5500 | 0.000 | 3 |
NaLi2BO3 (mp-560189) | 0.6789 | 0.000 | 4 |
K4Rb2Co2O5 (mp-504848) | 0.4760 | 0.000 | 4 |
K2Na4Co2O5 (mp-504963) | 0.6597 | 0.322 | 4 |
Rb2Na4Co2O5 (mp-504964) | 0.7015 | 0.000 | 4 |
K2Na4Be2O5 (mp-14324) | 0.4552 | 0.000 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Cs_sv K_sv Fe_pv O |
Final Energy/Atom-4.5547 eV |
Corrected Energy-67.1575 eV
Uncorrected energy = -59.2105 eV
Composition-based energy adjustment (-0.687 eV/atom x 5.0 atoms) = -3.4350 eV
Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV
Corrected energy = -67.1575 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)