Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZrSe2 + SrSe |
Band Gap0.167 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 289.5 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 275.2 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 137.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 325.7 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 234.1 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 253.3 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 253.3 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 206.4 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 206.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 289.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 253.3 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 108.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 253.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 180.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 180.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 145.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 289.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 217.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 137.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 325.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 289.5 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 325.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 180.9 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 292.6 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 206.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 217.1 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 217.1 |
GaP (mp-2490) | <1 1 1> | <0 1 1> | 275.2 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 206.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 275.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 217.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 1> | 137.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 292.6 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 175.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 289.5 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 325.7 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 289.5 |
PbSe (mp-2201) | <1 1 1> | <1 0 1> | 137.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 144.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 1> | 68.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 1> | 68.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 325.7 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 1> | 275.2 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 217.1 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 1> | 137.6 |
SiC (mp-11714) | <0 0 1> | <0 1 1> | 275.2 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 180.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 253.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 292.6 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 1> | 137.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlCdI3 (mp-27252) | 0.2503 | 0.017 | 3 |
CdInBr3 (mp-505222) | 0.2541 | 0.008 | 3 |
TlGeI3 (mp-29288) | 0.2180 | 0.016 | 3 |
SrZrS3 (mp-558760) | 0.1819 | 0.000 | 3 |
TlCdBr3 (mp-28219) | 0.2640 | 0.001 | 3 |
Ca5Mn2(NiO6)2 (mvc-13112) | 0.6088 | 0.106 | 4 |
CsK2BiCl6 (mp-571371) | 0.6611 | 0.000 | 4 |
MnSb6(Pb2S7)2 (mp-683891) | 0.6658 | 0.008 | 4 |
Sr3CaRu2O9 (mp-557111) | 0.6664 | 0.000 | 4 |
La2InCuSe5 (mp-21390) | 0.6681 | 0.006 | 4 |
Tl2Cl3 (mp-680294) | 0.7434 | 0.000 | 2 |
K3Na2LiTeO6 (mp-559875) | 0.6930 | 0.000 | 5 |
Ca2La2MgTi3O12 (mp-676461) | 0.7296 | 0.032 | 5 |
LiCaPrTeO6 (mp-40186) | 0.7056 | 0.024 | 5 |
CaPr2Ti2ZnO9 (mp-686602) | 0.6670 | 0.026 | 5 |
CaNd2Ti2ZnO9 (mp-677231) | 0.6782 | 0.034 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Zr_sv Se |
Final Energy/Atom-5.7401 eV |
Corrected Energy-114.8026 eV
-114.8026 eV = -114.8026 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)