Final Magnetic Moment0.964 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.265 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.121 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKC2N3 + K2CN2 + FeN + C |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 229.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 -1> | 293.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 266.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 171.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 286.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 229.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 266.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 224.8 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 283.0 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 293.6 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 293.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 171.9 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 293.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 283.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 114.6 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 266.6 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 94.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 229.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 286.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 132.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 177.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 149.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 224.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 132.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 264.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 149.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 224.8 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 224.8 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 229.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 132.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 224.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 224.8 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 226.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 286.5 |
Al (mp-134) | <1 0 0> | <0 1 0> | 286.5 |
Al (mp-134) | <1 1 0> | <0 1 1> | 94.3 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 229.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 293.6 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 132.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 105.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 -1> | 226.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 283.0 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 283.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 224.8 |
C (mp-66) | <1 0 0> | <0 1 1> | 283.0 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 293.6 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 286.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 266.6 |
Mg (mp-153) | <1 1 0> | <1 0 -1> | 293.6 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 149.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsI5F6 (mp-31020) | 0.6193 | 0.000 | 3 |
Sb2I2F11 (mp-27236) | 0.6193 | 0.017 | 3 |
As(IF2)3 (mp-27445) | 0.6344 | 0.000 | 3 |
Li5Br2N (mp-29025) | 0.6498 | 0.003 | 3 |
SbBr5F6 (mp-541259) | 0.6555 | 0.000 | 3 |
K3Co(CN)6 (mp-6219) | 0.1758 | 0.065 | 4 |
K3Fe(CN)6 (mp-621921) | 0.1339 | 0.124 | 4 |
K3Co(CN)6 (mp-680180) | 0.2189 | 0.071 | 4 |
K3Mn(CN)6 (mp-540801) | 0.1104 | 0.172 | 4 |
K3Cr(CN)6 (mp-645346) | 0.2647 | 0.158 | 4 |
TaF5 (mp-561197) | 0.7338 | 0.000 | 2 |
ZrF4 (mp-34260) | 0.7250 | 0.133 | 2 |
MoF5 (mp-555649) | 0.7080 | 0.078 | 2 |
NbF5 (mp-18687) | 0.7097 | 0.000 | 2 |
MoF5 (mp-608126) | 0.7032 | 0.078 | 2 |
K3CrC5N6O (mp-705039) | 0.2548 | 0.423 | 5 |
K2NaAg3(CN)6 (mp-6855) | 0.5557 | 0.207 | 5 |
Cs2KFe(CN)6 (mp-505660) | 0.5714 | 0.093 | 5 |
Cs2KCo(CN)6 (mp-505662) | 0.5664 | 0.021 | 5 |
Cs2RbFe(CN)6 (mp-505661) | 0.5467 | 0.097 | 5 |
AgSbH2C2(NF3)2 (mp-690698) | 0.7450 | 0.160 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Fe_pv C N |
Final Energy/Atom-7.4443 eV |
Corrected Energy-238.2187 eV
-238.2187 eV = -238.2187 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)