Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.045 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.649 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 225.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 260.3 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 260.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 225.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 271.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 81.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 203.6 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 162.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 163.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 270.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 180.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 216.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 324.5 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 244.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 316.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 316.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 163.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 162.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 173.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 244.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 211.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 260.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 324.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 216.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 163.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 162.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 293.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 270.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 162.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 293.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 293.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 195.6 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 270.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 163.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 90.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 271.4 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 70.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 225.8 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 293.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 67.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 203.6 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 135.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 203.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 135.5 |
BN (mp-984) | <1 1 0> | <1 0 1> | 163.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 260.3 |
LiNbO3 (mp-3731) | <1 1 1> | <1 1 0> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaReN3 (mp-989637) | 0.5474 | 0.000 | 3 |
SrTcN3 (mp-989627) | 0.5685 | 0.000 | 3 |
SrReN3 (mp-989623) | 0.5881 | 0.000 | 3 |
LaCrN3 (mp-989612) | 0.5494 | 0.000 | 3 |
K5V3O10 (mp-556791) | 0.5971 | 0.000 | 3 |
Na2CoP2O7 (mp-1013577) | 0.5783 | 0.022 | 4 |
Sr2Ni(PO4)2 (mp-557764) | 0.5916 | 0.000 | 4 |
Na2ZrSi2O7 (mp-558191) | 0.5469 | 0.000 | 4 |
K3V2(PO4)3 (mp-1022965) | 0.5818 | 0.029 | 4 |
K2Ca3Si3O10 (mp-1019747) | 0.5523 | 0.000 | 4 |
CaZnAsHO5 (mp-24018) | 0.2282 | 0.000 | 5 |
CaCoAsHO5 (mp-510721) | 0.1176 | 0.056 | 5 |
ZnAsHPbO5 (mp-510279) | 0.4146 | 0.000 | 5 |
CaMnSiHO5 (mp-25699) | 0.4258 | 0.011 | 5 |
CaAlSiHO5 (mp-24402) | 0.3244 | 0.005 | 5 |
NaCa3AlFe3(SiO3)8 (mp-743726) | 0.6860 | 0.021 | 6 |
NaCa3ScZn3(SiO3)8 (mp-693463) | 0.6954 | 0.029 | 6 |
NaCaScZn(SiO3)4 (mp-684991) | 0.6836 | 0.019 | 6 |
NaCa2ScZn2(SiO3)6 (mp-534778) | 0.6931 | 0.025 | 6 |
KCa5Mg5Al(SiO3)12 (mp-534793) | 0.6782 | 0.025 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Ni_pv As H O |
Final Energy/Atom-5.9064 eV |
Corrected Energy-235.3317 eV
-235.3317 eV = -212.6299 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)