Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.227 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi4Rh + BiI3 |
Band Gap0.516 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 199.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 137.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 113.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 137.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 226.5 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 199.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 226.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 211.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 137.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 113.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 133.3 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 281.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 211.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 226.5 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 128.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 128.5 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 226.5 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 133.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 226.5 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 226.5 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 226.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 281.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 281.5 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 0> | 281.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 281.5 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 281.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 140.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 257.1 |
BN (mp-984) | <1 1 1> | <0 1 1> | 133.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 128.5 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 137.5 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 226.5 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 281.5 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 257.1 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 226.5 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 226.5 |
NaCl (mp-22862) | <1 1 0> | <1 0 -1> | 137.5 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 113.3 |
Ge (mp-32) | <1 1 0> | <1 0 -1> | 137.5 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 113.3 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 1> | 133.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 281.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 0> | 211.1 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 281.5 |
MgF2 (mp-1249) | <0 0 1> | <1 0 1> | 199.5 |
SrTiO3 (mp-4651) | <1 0 0> | <0 0 1> | 226.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2PbF8 (mp-676816) | 0.6705 | 0.030 | 3 |
BiPtPb3 (mp-680530) | 0.6652 | 0.002 | 3 |
Bi9Ir2I3 (mp-680182) | 0.4718 | 0.000 | 3 |
Bi9Rh2Br3 (mp-680173) | 0.4566 | 0.029 | 3 |
Ni6Ge2B (mp-1078540) | 0.6432 | 0.000 | 3 |
CeSb(SBr)2 (mp-680417) | 0.6895 | 0.003 | 4 |
LaSb(SBr)2 (mp-680334) | 0.6864 | 0.000 | 4 |
MgSi (mp-1073722) | 0.5831 | 0.158 | 2 |
MgSi (mp-1073754) | 0.5559 | 0.158 | 2 |
Mg4Si3 (mp-1074517) | 0.5830 | 0.159 | 2 |
Mg2Si (mp-1074636) | 0.5892 | 0.199 | 2 |
Mg7Si4 (mp-1074925) | 0.5874 | 0.219 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi Rh_pv I |
Final Energy/Atom-4.1067 eV |
Corrected Energy-114.9869 eV
-114.9869 eV = -114.9869 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)