Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-3.082 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.905 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421m [113] |
HallP 4 2ab |
Point Group42m |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 136.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 136.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 228.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 248.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 64.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 129.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 228.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 248.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 136.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 228.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 91.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 129.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 193.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 228.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 193.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 273.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 228.2 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 94.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 228.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 91.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 136.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 193.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 273.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 193.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 165.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 193.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 182.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 136.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 193.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 228.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 273.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 283.9 |
BN (mp-984) | <1 0 1> | <1 1 0> | 322.7 |
BN (mp-984) | <1 1 1> | <1 0 0> | 136.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 1> | 248.7 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 228.2 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 248.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 136.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 248.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 82.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 45.6 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 64.5 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 136.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 69.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 136.9 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 319.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 69.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 319.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 228.2 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 193.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2Si2CuO7 (mp-11613) | 0.2074 | 0.040 | 4 |
Ba2MgSi2O7 (mp-9338) | 0.0378 | 0.000 | 4 |
Eu2MgSi2O7 (mp-982662) | 0.2906 | 0.000 | 4 |
Sr2Si2CuO7 (mp-15748) | 0.2215 | 0.050 | 4 |
Sr2MgSi2O7 (mp-6564) | 0.2844 | 0.000 | 4 |
P2O5 (mp-2452) | 0.7468 | 0.000 | 2 |
Tm2P4O13 (mp-772744) | 0.5797 | 0.041 | 3 |
Er2P4O13 (mp-773003) | 0.5808 | 0.045 | 3 |
LuP5O14 (mp-773020) | 0.5522 | 0.013 | 3 |
Lu2P4O13 (mp-773016) | 0.5849 | 0.061 | 3 |
DyP5O14 (mp-779893) | 0.5601 | 0.009 | 3 |
K2BiPWO8 (mp-566769) | 0.7328 | 0.001 | 5 |
K2BiMoPO8 (mp-566924) | 0.7300 | 0.000 | 5 |
Ba2ZnGe2S6O (mp-17244) | 0.4749 | 0.000 | 5 |
SrZnP2(HO4)2 (mp-697018) | 0.6541 | 0.850 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points9 |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Ba_sv Co Si O |
Final Energy/Atom-7.2129 eV |
Corrected Energy-186.6908 eV
-186.6908 eV = -173.1107 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)