Final Magnetic Moment10.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.774 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.131 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 |
Band Gap1.446 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 199.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 137.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 145.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 119.7 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 1> | 242.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 119.7 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 47.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 193.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 27.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 279.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 119.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 82.4 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 278.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 242.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 159.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 247.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 82.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 279.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 116.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 137.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 116.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 142.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 329.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 155.1 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 242.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 119.7 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 142.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 119.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 290.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 159.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 247.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 159.5 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 319.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 278.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 278.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 339.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 193.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 278.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 278.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 82.4 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 232.7 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 279.2 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 79.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 219.9 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 310.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 155.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 47.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 142.6 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 302.3 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 222.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-754361) | 0.2976 | 0.097 | 3 |
YbSmO3 (mp-752596) | 0.2257 | 0.146 | 3 |
SmYO3 (mp-755685) | 0.2691 | 0.064 | 3 |
Zr2N2O (mp-776239) | 0.2975 | 0.099 | 3 |
LaBiO3 (mp-768310) | 0.3002 | 0.035 | 3 |
Li3Nb4NiO12 (mp-772009) | 0.4032 | 0.089 | 4 |
Li3Nb4FeO12 (mp-771984) | 0.4035 | 0.030 | 4 |
Mg2VWO6 (mvc-5881) | 0.3741 | 0.018 | 4 |
Mg2TiWO6 (mvc-5939) | 0.3980 | 0.128 | 4 |
InNi2SbO6 (mp-1078367) | 0.3920 | 0.000 | 4 |
Y2O3 (mp-775906) | 0.1417 | 0.063 | 2 |
Cr2O3 (mp-776526) | 0.1476 | 0.047 | 2 |
Al2O3 (mp-1938) | 0.0657 | 0.093 | 2 |
Rh2S3 (mp-17173) | 0.1513 | 0.000 | 2 |
Ca3N2 (mp-568293) | 0.0652 | 0.032 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.5912 | 0.083 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.6981 | 0.081 | 5 |
Li4MnV2WO12 (mp-773239) | 0.7079 | 0.088 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6618 | 0.054 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.7071 | 0.181 | 5 |
Explore more synthesis descriptions for materials of composition Fe2O3.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O |
Final Energy/Atom-6.6186 eV |
Corrected Energy-162.6626 eV
-162.6626 eV = -132.3711 eV (uncorrected energy) - 21.8640 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)