Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.420 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZn2P2O7 |
Band Gap3.628 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 167.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 232.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 172.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 167.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 310.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 310.0 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 172.2 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 195.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 172.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 232.5 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 310.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 232.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 167.1 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 155.0 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 310.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 232.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 310.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 232.5 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 232.5 |
SiC (mp-11714) | <1 0 1> | <1 1 0> | 197.3 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 155.0 |
Au (mp-81) | <1 1 0> | <1 0 1> | 195.4 |
C (mp-48) | <0 0 1> | <1 0 0> | 232.5 |
C (mp-48) | <1 1 1> | <1 0 0> | 310.0 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 -1> | 172.2 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 232.5 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 197.3 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 232.5 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 310.0 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 195.4 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 -1> | 172.2 |
GaTe (mp-542812) | <1 0 1> | <1 0 1> | 195.4 |
Ge (mp-32) | <1 1 1> | <1 0 0> | 232.5 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 167.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni6P7O24 (mp-504372) | 0.4313 | 0.009 | 3 |
Co2P2O7 (mp-25739) | 0.2798 | 0.059 | 3 |
Ni2P2O7 (mp-745012) | 0.3304 | 0.000 | 3 |
AlPO4 (mp-1019512) | 0.5004 | 0.085 | 3 |
Zn2As2O7 (mp-781624) | 0.4346 | 0.013 | 3 |
ZnCoP2O7 (mvc-13193) | 0.2661 | 0.090 | 4 |
MgCoP2O7 (mvc-1216) | 0.2546 | 0.108 | 4 |
VZnP2O7 (mvc-1230) | 0.2529 | 0.101 | 4 |
MgVP2O7 (mvc-1224) | 0.2584 | 0.020 | 4 |
ZnFeP2O7 (mvc-1240) | 0.2640 | 0.185 | 4 |
LiV3Fe2CuO12 (mp-767459) | 0.6938 | 2.323 | 5 |
Al2CuSi2O7F2 (mp-557084) | 0.7150 | 0.034 | 5 |
Li2V2SiGeO10 (mp-771932) | 0.7176 | 0.046 | 5 |
LiMgIn(MoO4)3 (mp-566467) | 0.6516 | 0.000 | 5 |
LiMnVP2(O4F)2 (mp-778336) | 0.6976 | 0.001 | 6 |
LiVFeP2(O4F)2 (mp-777635) | 0.7162 | 0.026 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn P O |
Final Energy/Atom-6.3351 eV |
Corrected Energy-447.6151 eV
-447.6151 eV = -418.1189 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)