Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.176 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 260.5 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 80.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 325.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 65.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 282.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 108.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 140.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 282.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 161.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 195.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 347.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 347.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 86.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 65.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 238.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 347.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 347.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 86.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 260.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 260.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 282.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 282.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 260.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 282.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 347.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 347.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 86.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 65.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 173.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 369.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 86.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 21.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 151.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 80.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 151.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 347.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 282.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 217.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 80.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 282.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 347.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 347.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 86.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YMg2Cu9 (mp-13218) | 0.0302 | 0.000 | 3 |
SmMg2Cu9 (mp-13222) | 0.0375 | 0.000 | 3 |
HoMg2Cu9 (mp-13226) | 0.0320 | 0.000 | 3 |
YbMg2Cu9 (mp-13227) | 0.0588 | 0.000 | 3 |
DyMg2Cu9 (mp-13225) | 0.0233 | 0.000 | 3 |
PuNi3 (mp-636403) | 0.2707 | 0.000 | 2 |
HoFe3 (mp-30634) | 0.3276 | 0.000 | 2 |
ErFe3 (mp-569783) | 0.3224 | 0.000 | 2 |
YbCo3 (mp-1095601) | 0.3022 | 0.006 | 2 |
ThFe3 (mp-1095695) | 0.3302 | 0.205 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Mg_pv Cu_pv |
Final Energy/Atom-3.9033 eV |
Corrected Energy-93.6800 eV
-93.6800 eV = -93.6800 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)