Final Magnetic Moment0.996 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.668 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsHSO4 + CuO + H2O |
Band Gap0.666 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 81.8 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 255.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 81.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 122.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 233.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 291.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 175.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 291.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 163.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.5 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 291.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 291.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 244.9 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 291.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 127.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 122.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 291.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 291.7 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 291.7 |
BN (mp-984) | <0 0 1> | <1 0 1> | 164.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 245.3 |
Al (mp-134) | <1 0 0> | <1 0 1> | 164.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 163.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 245.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 291.7 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 291.7 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 291.7 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 175.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 163.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 163.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 291.7 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 175.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 233.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 163.5 |
Au (mp-81) | <1 1 0> | <0 1 0> | 291.7 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 245.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 163.5 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 291.7 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 175.0 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 291.7 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 0> | 291.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 -1> | 255.5 |
CaCO3 (mp-3953) | <1 0 1> | <0 1 0> | 175.0 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 291.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 291.7 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 0> | 291.7 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 163.5 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 245.3 |
WS2 (mp-224) | <1 0 1> | <1 1 0> | 135.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrH6SO7 (mp-745180) | 0.5375 | 0.026 | 4 |
MgH2SeO5 (mp-23966) | 0.5552 | 0.000 | 4 |
VH10SO10 (mp-745140) | 0.5625 | 0.001 | 4 |
MnAsH2O5 (mp-25557) | 0.5615 | 0.000 | 4 |
MnPH2O5 (mp-25046) | 0.5262 | 0.000 | 4 |
Tl2CuH12(SO7)2 (mp-24196) | 0.3985 | 0.000 | 5 |
Rb2CuH12(SO7)2 (mp-24197) | 0.3663 | 0.005 | 5 |
Rb2CuH12(SeO7)2 (mp-510018) | 0.4448 | 0.000 | 5 |
Cs2CuH12(SO7)2 (mp-658087) | 0.3045 | 0.008 | 5 |
Rb2CuH12(SO7)2 (mp-559981) | 0.4004 | 0.005 | 5 |
K2FePH5(CO5)2 (mp-604118) | 0.7210 | 0.119 | 6 |
CsKTeH6SO10 (mp-559375) | 0.7252 | 0.000 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.7488 | 0.072 | 6 |
Be2CoH20N2(O3F4)2 (mp-25732) | 0.7417 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Cu_pv H S O |
Final Energy/Atom-5.2535 eV |
Corrected Energy-348.0330 eV
-348.0330 eV = -325.7151 eV (uncorrected energy) - 22.3180 eV (MP Anion Correction)
|