Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.290 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.941 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPban [50] |
HallP 2 2 1ab |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 312.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 278.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 312.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 187.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 185.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 111.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 124.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 195.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 187.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 312.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 111.9 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 92.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 62.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 223.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 312.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 187.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 195.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 187.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 195.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 187.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 249.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 187.3 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 278.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 187.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 278.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 195.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 278.7 |
BN (mp-984) | <1 0 1> | <0 1 0> | 278.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 195.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 187.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 111.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 249.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 223.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 62.4 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 223.8 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 312.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 312.1 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 249.7 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 278.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 124.8 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 278.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 62.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 223.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 187.3 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 278.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 312.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 187.3 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 124.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 62.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 124.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2SeO3 (mp-557637) | 0.5356 | 0.000 | 3 |
Hg2SeO3 (mp-555918) | 0.5819 | 0.006 | 3 |
Tl3AsS3 (mp-9791) | 0.5780 | 0.010 | 3 |
Rb3SbO3 (mp-757084) | 0.5820 | 0.055 | 3 |
Ag2SeO3 (mp-16913) | 0.5531 | 0.000 | 3 |
BiTeIO3 (mp-559332) | 0.5530 | 0.006 | 4 |
CoSb2Br2O3 (mp-561493) | 0.6947 | 0.000 | 4 |
Ag2Hg(SeO3)2 (mp-558763) | 0.7024 | 0.011 | 4 |
LaNiSnH (mp-510577) | 0.7147 | 0.000 | 4 |
AgAsPbS3 (mp-22665) | 0.5725 | 0.000 | 4 |
XeO3 (mp-562054) | 0.7161 | 0.938 | 2 |
GeO2 (mp-20893) | 0.7264 | 1.561 | 2 |
BiS2 (mp-971673) | 0.7482 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Te O |
Final Energy/Atom-4.7160 eV |
Corrected Energy-243.2231 eV
-243.2231 eV = -226.3681 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)