Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.128 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.150 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap4.835 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4122 [98] |
HallI 4bw 2bw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 90.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 161.1 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 71.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 215.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 272.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 96.6 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 181.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 215.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 128.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 90.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 161.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 64.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 161.1 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 215.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 32.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 90.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 289.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 32.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 90.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 225.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 193.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 257.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.2 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 289.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 287.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 289.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 322.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 322.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 225.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 257.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 354.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 161.1 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 272.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 257.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 193.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 322.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 32.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 225.5 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 181.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 71.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 1> | 289.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 289.9 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 128.5 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 272.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 90.9 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 161.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 161.1 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 181.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 289.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuPO3 (mp-772192) | 0.7197 | 0.073 | 3 |
GaAsO4 (mp-3996) | 0.7378 | 0.000 | 3 |
VBO4 (mp-771386) | 0.6643 | 0.068 | 3 |
LiFeF4 (mp-777020) | 0.7250 | 0.095 | 3 |
AlPO4 (mp-560815) | 0.6664 | 0.030 | 3 |
RbMgPO4 (mp-975103) | 0.7260 | 0.000 | 4 |
Na2Zn(SiO3)2 (mp-558580) | 0.7361 | 0.008 | 4 |
CsLiCrO4 (mp-615884) | 0.6868 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.7038 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.7106 | 0.000 | 4 |
SiO2 (mp-561291) | 0.4767 | 0.146 | 2 |
SiO2 (mp-555497) | 0.4332 | 0.250 | 2 |
SiO2 (mp-559860) | 0.4468 | 0.160 | 2 |
SiO2 (mp-560954) | 0.4465 | 0.169 | 2 |
CeSe2 (mp-1080288) | 0.3800 | 0.520 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.7666 eV |
Corrected Energy-98.8180 eV
-98.8180 eV = -93.1997 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)