NaTaN2

ID:

mp-5475

DOI:

10.17188/1267310


Tags: Sodium tantalum nitride (1/1/2) Sodium tantalum dinitride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-1.097 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.91 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.277 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <0 0 1> 0.000 264.7
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.001 264.7
LaF3 (mp-905) <0 0 1> <0 0 1> 0.002 136.6
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.011 59.8
KCl (mp-23193) <1 1 1> <0 0 1> 0.020 213.5
C (mp-48) <1 0 1> <1 1 0> 0.028 279.3
AlN (mp-661) <1 1 0> <0 0 1> 0.028 136.6
AlN (mp-661) <0 0 1> <0 0 1> 0.051 8.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.059 93.1
C (mp-48) <1 1 0> <1 0 0> 0.060 268.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.067 76.9
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.076 85.4
CdTe (mp-406) <1 1 1> <0 0 1> 0.088 76.9
MoSe2 (mp-1634) <1 1 1> <1 0 0> 0.091 268.7
CdSe (mp-2691) <1 1 1> <0 0 1> 0.095 264.7
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.096 25.6
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.104 215.0
PbSe (mp-2201) <1 0 0> <0 0 1> 0.108 273.3
Au (mp-81) <1 1 1> <0 0 1> 0.132 213.5
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.142 333.1
GaSb (mp-1156) <1 0 0> <0 0 1> 0.144 273.3
ZnO (mp-2133) <0 0 1> <0 0 1> 0.148 111.0
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.151 85.4
AlN (mp-661) <1 0 1> <1 0 1> 0.156 54.4
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.158 93.1
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.167 162.3
BN (mp-984) <0 0 1> <0 0 1> 0.169 102.5
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.179 162.3
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.179 111.0
CdSe (mp-2691) <1 0 0> <0 0 1> 0.182 273.3
GaTe (mp-542812) <1 0 0> <0 0 1> 0.183 136.6
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.184 273.3
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.187 264.7
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.208 93.1
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.209 76.9
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.221 128.1
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.233 333.1
BN (mp-984) <1 1 1> <1 0 0> 0.238 268.7
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.251 136.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.259 273.3
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.265 268.7
Ag (mp-124) <1 1 1> <0 0 1> 0.268 213.5
GaTe (mp-542812) <0 0 1> <0 0 1> 0.269 298.9
Ag (mp-124) <1 1 0> <0 0 1> 0.271 170.8
CdS (mp-672) <1 0 0> <1 0 0> 0.285 322.5
WS2 (mp-224) <1 1 0> <0 0 1> 0.287 239.1
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.288 136.6
Mg (mp-153) <1 0 0> <1 0 0> 0.296 215.0
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.297 322.5
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.299 59.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
407 80 36 2 0 0
80 407 36 -2 0 0
36 36 195 -0 0 0
2 -2 -0 50 0 0
0 0 0 0 50 2
0 0 0 0 2 164
Compliance Tensor Sij (10-12Pa-1)
2.6 -0.5 -0.4 -0.1 0 0
-0.5 2.6 -0.4 0.1 0 0
-0.4 -0.4 5.3 0 0 0
-0.1 0.1 0 20 0 0
0 0 0 0 20 -0.3
0 0 0 0 -0.3 6.1
Shear Modulus GV
110 GPa
Bulk Modulus KV
146 GPa
Shear Modulus GR
81 GPa
Bulk Modulus KR
126 GPa
Shear Modulus GVRH
96 GPa
Bulk Modulus KVRH
136 GPa
Elastic Anisotropy
1.93
Poisson's Ratio
0.22

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
60
U Values
--
Pseudopotentials
VASP PAW: N Na_pv Ta_pv
Final Energy/Atom
-8.3645 eV
Corrected Energy
-33.4579 eV
-33.4579 eV = -33.4579 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations

User Data

dtu

Authors:
name conditions value ref
band gap
type
indirect
method
Kohn-Sham
functional
GLLB-SC
1.18 eV
band gap
type
direct
method
Kohn-Sham
functional
GLLB-SC
1.63 eV
band gap
type
indirect
method
quasiparticle
functional
GLLB-SC
1.56 eV
band gap
type
direct
method
quasiparticle
functional
GLLB-SC
2.01 eV
derivative discontinuity
functional
GLLB-SC
0.38 eV

Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 67346
  • 67347
  • 76382

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)