material

Ca(CuSi)2

ID:

mp-5486

DOI:

10.17188/1267331


Tags: Calcium copper silicide (1/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.401 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.55 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 25314 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <0 0 1> 0.001 81.9
Cu (mp-30) <1 0 0> <0 0 1> 0.002 65.5
Mg (mp-153) <0 0 1> <1 1 0> 0.004 113.9
Ni (mp-23) <1 1 1> <1 1 0> 0.007 170.9
TiO2 (mp-390) <1 1 1> <1 0 1> 0.007 217.4
Ge(Bi3O5)4 (mp-23352) <1 0 0> <0 0 1> 0.008 213.0
AlN (mp-661) <1 0 1> <0 0 1> 0.009 196.6
Al (mp-134) <1 0 0> <0 0 1> 0.009 16.4
GaSe (mp-1943) <0 0 1> <1 1 0> 0.009 113.9
TiO2 (mp-390) <0 0 1> <0 0 1> 0.014 131.1
KP(HO2)2 (mp-23959) <0 1 0> <1 0 1> 0.015 304.4
GaN (mp-804) <1 0 0> <1 0 0> 0.015 201.4
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.021 32.8
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.021 113.9
WS2 (mp-224) <0 0 1> <1 1 0> 0.022 113.9
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.031 227.9
BN (mp-984) <0 0 1> <1 1 0> 0.033 113.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.035 16.4
C (mp-48) <1 1 1> <1 0 0> 0.038 201.4
C (mp-48) <1 1 0> <1 0 0> 0.039 201.4
Al (mp-134) <1 1 1> <1 1 0> 0.043 57.0
GaAs (mp-2534) <1 0 0> <0 0 1> 0.043 32.8
C (mp-48) <0 0 1> <1 1 1> 0.046 177.8
KP(HO2)2 (mp-23959) <0 0 1> <1 0 1> 0.055 304.4
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 0.063 304.4
NaCl (mp-22862) <1 0 0> <0 0 1> 0.065 32.8
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.075 227.9
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.075 311.3
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.075 284.9
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.077 147.4
AlN (mp-661) <1 1 0> <1 0 1> 0.083 217.4
NaCl (mp-22862) <1 1 0> <1 1 0> 0.085 227.9
CdS (mp-672) <1 0 0> <0 0 1> 0.087 262.1
LiGaO2 (mp-5854) <1 1 0> <1 1 0> 0.088 341.8
KTaO3 (mp-3614) <1 1 1> <1 1 0> 0.089 57.0
YAlO3 (mp-3792) <1 1 1> <0 0 1> 0.089 311.3
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.091 174.0
Ge (mp-32) <1 0 0> <0 0 1> 0.095 32.8
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.096 282.0
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.096 177.8
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.097 147.4
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.103 296.4
Si (mp-149) <1 0 0> <0 0 1> 0.104 147.4
ZnO (mp-2133) <0 0 1> <1 1 0> 0.107 57.0
LiF (mp-1138) <1 1 1> <1 1 0> 0.109 57.0
LaF3 (mp-905) <1 0 0> <0 0 1> 0.110 213.0
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.112 284.9
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.114 113.9
ZnO (mp-2133) <1 1 0> <1 0 1> 0.114 304.4
Cu (mp-30) <1 1 1> <1 1 1> 0.117 296.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
173 29 66 0 0 0
29 173 66 0 0 0
66 66 170 0 0 0
0 0 0 58 0 0
0 0 0 0 58 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
6.8 -0.1 -2.6 0 0 0
-0.1 6.8 -2.6 0 0 0
-2.6 -2.6 7.9 0 0 0
0 0 0 17.4 0 0
0 0 0 0 17.4 0
0 0 0 0 0 24.6
Shear Modulus GV
55 GPa
Bulk Modulus KV
93 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
92 GPa
Shear Modulus GVRH
54 GPa
Bulk Modulus KVRH
93 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.26

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nd(CuSi)2 (mp-2877) 0.0715 0.000 3
Eu(ZnGe)2 (mp-20771) 0.0269 0.008 3
Sm(AsPd)2 (mp-570216) 0.0176 0.040 3
Ca(ZnGe)2 (mp-13911) 0.0511 0.003 3
Nd(AsPd)2 (mp-12060) 0.0649 0.000 3
La3Cu4(P2O)2 (mp-6309) 0.5898 0.000 4
YbGa4 (mp-1088) 0.1385 0.000 2
CaGa4 (mp-1976) 0.1230 0.000 2
SrGa4 (mp-1827) 0.1170 0.000 2
BaAl4 (mp-1903) 0.0731 0.000 2
BaIn4 (mp-22687) 0.1090 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Cu_pv Si
Final Energy/Atom
-4.6095 eV
Corrected Energy
-22.9054 eV
Uncorrected energy = -23.0474 eV Composition-based energy adjustment (0.071 eV/atom x 2.0 atoms) = 0.1420 eV Corrected energy = -22.9054 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 25314
  • 619236
  • 619238
Submitted by
User remarks:
  • Calcium copper silicide (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)