Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.935 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 1335 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <1 0 0> 0.002 277.8
Au (mp-81) <1 1 0> <1 1 0> 0.003 49.1
Au (mp-81) <1 0 0> <1 0 0> 0.003 34.7
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.004 60.1
Ag (mp-124) <1 1 0> <1 1 0> 0.005 49.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.005 173.6
GaSe (mp-1943) <0 0 1> <1 1 1> 0.006 240.6
Ag (mp-124) <1 0 0> <1 0 0> 0.006 34.7
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.011 147.3
Cu (mp-30) <1 1 0> <1 1 0> 0.012 147.3
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.013 277.8
GaTe (mp-542812) <1 0 0> <1 1 1> 0.014 180.4
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.015 312.5
GaN (mp-804) <0 0 1> <1 1 1> 0.018 240.6
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.021 277.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.022 173.6
TePb (mp-19717) <1 0 0> <1 0 0> 0.030 173.6
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.037 343.7
PbSe (mp-2201) <1 0 0> <1 0 0> 0.037 312.5
LaF3 (mp-905) <0 0 1> <1 1 1> 0.039 180.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.049 138.9
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.053 277.8
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.060 173.6
WS2 (mp-224) <0 0 1> <1 1 1> 0.062 240.6
GaN (mp-804) <1 0 1> <1 0 0> 0.062 208.3
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.063 240.6
GaSb (mp-1156) <1 0 0> <1 0 0> 0.066 312.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.078 312.5
GaTe (mp-542812) <0 0 1> <1 1 1> 0.081 300.7
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.082 60.1
CsI (mp-614603) <1 0 0> <1 0 0> 0.093 312.5
CdSe (mp-2691) <1 0 0> <1 0 0> 0.095 312.5
Au (mp-81) <1 1 1> <1 0 0> 0.096 243.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.099 294.6
ZnO (mp-2133) <0 0 1> <1 1 1> 0.103 180.4
CdTe (mp-406) <1 0 0> <1 0 0> 0.107 173.6
CdS (mp-672) <1 0 0> <1 0 0> 0.122 173.6
GaN (mp-804) <1 1 1> <1 0 0> 0.123 277.8
Te2W (mp-22693) <0 1 1> <1 1 0> 0.129 294.6
Mg (mp-153) <1 0 1> <1 0 0> 0.129 208.3
InSb (mp-20012) <1 0 0> <1 0 0> 0.130 173.6
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.132 312.5
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.135 277.8
WS2 (mp-224) <1 1 1> <1 1 1> 0.135 240.6
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.136 277.8
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.149 180.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.158 138.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.161 173.6
AlN (mp-661) <1 1 1> <1 1 0> 0.165 196.4
Ag (mp-124) <1 1 1> <1 0 0> 0.168 243.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
148 23 23 0 0 0
23 148 23 0 0 0
23 23 148 0 0 0
0 0 0 23 0 0
0 0 0 0 23 0
0 0 0 0 0 23
Compliance Tensor Sij (10-12Pa-1)
7 -0.9 -0.9 0 0 0
-0.9 7 -0.9 0 0 0
-0.9 -0.9 7 0 0 0
0 0 0 43.7 0 0
0 0 0 0 43.7 0
0 0 0 0 0 43.7
Shear Modulus GV
39 GPa
Bulk Modulus KV
65 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
65 GPa
Shear Modulus GVRH
35 GPa
Bulk Modulus KVRH
65 GPa
Elastic Anisotropy
1.32
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.039 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
NdBi (mp-23300) 0.0000 0.000 2
PuSb (mp-2566) 0.0000 0.000 2
LuTe (mp-1254) 0.0000 0.042 2
SnSe (mp-2693) 0.0000 0.000 2
ThSb (mp-1751) 0.0000 0.000 2
As (mp-10) 0.0000 0.126 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.393 1
C (mp-998866) 0.0000 2.763 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sc_sv Sb
Final Energy/Atom
-6.1656 eV
Corrected Energy
-12.3312 eV
-12.3312 eV = -12.3312 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 157507
  • 651513
  • 651514
  • 164629
  • 1335
Submitted by
User remarks:
  • Scandium antimonide - B1 (LP)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)