material

InCuO2

ID:

mp-549158

DOI:

10.17188/1267370


Tags: Copper(I) indium oxide Copper(I) indium dioxide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.492 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.005 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.14 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cu2O + In2O3
Band Gap
0.252 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.000 68.4
C (mp-48) <0 0 1> <0 0 1> 0.001 68.4
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.002 68.4
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.003 68.4
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.007 273.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.011 303.1
InSb (mp-20012) <1 1 1> <0 0 1> 0.018 303.1
Si (mp-149) <1 1 1> <0 0 1> 0.022 156.4
Cu (mp-30) <1 1 1> <0 0 1> 0.025 68.4
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.025 156.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.027 156.4
GaN (mp-804) <0 0 1> <0 0 1> 0.028 117.3
InP (mp-20351) <1 1 1> <0 0 1> 0.029 185.7
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.030 127.1
C (mp-66) <1 0 0> <0 0 1> 0.032 205.3
GaP (mp-2490) <1 0 0> <1 1 0> 0.033 271.0
PbS (mp-21276) <1 1 1> <0 0 1> 0.035 185.7
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.039 264.0
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.040 244.4
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.042 342.2
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.047 117.3
CdS (mp-672) <0 0 1> <0 0 1> 0.052 185.7
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.059 88.0
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.061 156.4
LiAlO2 (mp-3427) <0 0 1> <1 1 0> 0.062 135.5
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.064 185.7
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.068 264.0
C (mp-48) <1 1 0> <0 0 1> 0.069 234.6
CaF2 (mp-2741) <1 0 0> <1 1 0> 0.077 271.0
MgO (mp-1265) <1 1 1> <0 0 1> 0.080 127.1
GaSe (mp-1943) <1 0 0> <1 0 0> 0.083 273.8
PbS (mp-21276) <1 1 0> <1 0 1> 0.090 201.6
GaSb (mp-1156) <1 1 0> <0 0 1> 0.091 273.7
CdWO4 (mp-19387) <1 1 0> <1 1 0> 0.092 203.3
TeO2 (mp-2125) <1 0 1> <0 0 1> 0.092 78.2
PbSe (mp-2201) <1 1 0> <0 0 1> 0.093 273.7
CdSe (mp-2691) <1 1 0> <0 0 1> 0.094 273.7
GaP (mp-2490) <1 1 0> <0 0 1> 0.095 342.2
GaAs (mp-2534) <1 1 0> <0 0 1> 0.096 234.6
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.100 121.0
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.101 185.7
InSb (mp-20012) <1 1 0> <0 0 1> 0.103 312.8
LiF (mp-1138) <1 1 0> <0 0 1> 0.107 117.3
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.108 117.3
TePb (mp-19717) <1 1 1> <0 0 1> 0.108 303.1
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.109 234.6
MoSe2 (mp-1634) <1 0 0> <0 0 1> 0.110 156.4
CdTe (mp-406) <1 1 0> <0 0 1> 0.110 312.8
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.112 97.8
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.112 342.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
167 70 93 0 0 0
70 167 93 0 0 0
93 93 308 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 49
Compliance Tensor Sij (10-12Pa-1)
7.9 -2.4 -1.7 0 0 0
-2.4 7.9 -1.7 0 0 0
-1.7 -1.7 4.2 0 0 0
0 0 0 54.3 0 0
0 0 0 0 54.3 0
0 0 0 0 0 20.6
Shear Modulus GV
43 GPa
Bulk Modulus KV
128 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
116 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
122 GPa
Elastic Anisotropy
2.12
Poisson's Ratio
0.36

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.77 -0.00 0.00
-0.00 5.77 0.00
0.00 0.00 4.98
Dielectric Tensor εij (total)
9.81 -0.00 0.00
-0.00 9.81 0.00
0.00 0.00 7.27
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.50
Polycrystalline dielectric constant εpoly
(total)
8.96
Refractive Index n
2.35
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaHgO2 (mp-7041) 0.0230 0.000 3
ScCuO2 (mp-3642) 0.0720 0.000 3
InCuO2 (mp-20930) 0.0047 0.005 3
YbAgO2 (mp-13166) 0.0760 0.129 3
ScCuO2 (mp-4636) 0.0718 0.001 3
CeSe2 (mp-1080306) 0.7118 0.189 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: In_d Cu_pv O
Final Energy/Atom
-5.3277 eV
Corrected Energy
-45.3698 eV
Uncorrected energy = -42.6218 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Corrected energy = -45.3698 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 95670
  • 186620
Submitted by
User remarks:
  • Copper(I) indium oxide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)